@ARTICLE{Endler:10068,
author = {Endler, C and Leonide, A. and Weber, A. and Tietz, F. and
Ivers-Tiffée, E.},
title = {{T}ime-dependent electrode performance changes in
intermediate temperature solid oxide fuel cells},
journal = {Journal of the Electrochemical Society},
volume = {157},
issn = {0013-4651},
address = {Pennington, NJ},
publisher = {Electrochemical Society},
reportid = {PreJuSER-10068},
pages = {B292 - B298},
year = {2010},
note = {Record converted from VDB: 12.11.2012},
abstract = {This study gives evidence that the time-dependent
performance changes in anode supported cells for
intermediate-temperature solid oxide fuel cells is
essentially influenced by the mixed ionic-electronic
conducting (MIEC) cathode. The impedance spectra recorded
during 700 h of operation at 750 degrees C were interpreted
using an appropriate equivalent circuit model by (i) a
distribution of relaxation time analysis followed by (ii) a
complex nonlinear least squares fit. Four electrode
polarization processes were separated by selective
experimental parameters. The cathodic part, initially the
smallest, is only discovered among the anodic contributions
by a change in fuel gas composition from H-2-H2O to CO-CO2
and increases by $310\%$ (15 m cm(2) at 11 h, 62 m cm(2) at
700 h). A Sr (and Co) depletion of the MIEC cathode
composition La0.58Sr0.4Co0.2Fe0.8O3-delta possibly caused
this degradation. The anodic polarization has a proportion
of $92\%$ at the start and decreases to $73\%$ (168 m cm(2)
at 11 h, 173 m cm(2) at 700 h). The anode charge-transfer
reaction initially causes $60\%$ of the total polarization
losses and $50\%$ after 700 h. This is assigned to a change
in the triple phase boundary and/or a degradation in ionic
conductivity in the anode functional layer. The gas
diffusion polarization remains constant at 58 m cm(2).},
keywords = {J (WoSType)},
cin = {IEF-1},
ddc = {540},
cid = {I:(DE-Juel1)VDB809},
pnm = {Rationelle Energieumwandlung / SOFC - Solid Oxide Fuel Cell
(SOFC-20140602)},
pid = {G:(DE-Juel1)FUEK402 / G:(DE-Juel1)SOFC-20140602},
shelfmark = {Electrochemistry / Materials Science, Coatings $\&$ Films},
typ = {PUB:(DE-HGF)16},
UT = {WOS:000273222700036},
doi = {10.1149/1.3270047},
url = {https://juser.fz-juelich.de/record/10068},
}