001016760 245__ $$aDual-Salts Electrolyte with Fluoroethylene Carbonate Additive for High-Voltage Li-Metal Batteries
001016760 260__ $$aBasel$$bMDPI$$c2023
001016760 3367_ $$2DRIVER$$aarticle
001016760 3367_ $$2DataCite$$aOutput Types/Journal article
001016760 3367_ $$0PUB:(DE-HGF)16$$2PUB:(DE-HGF)$$aJournal Article$$bjournal$$mjournal$$s1698383069_20388
001016760 3367_ $$2BibTeX$$aARTICLE
001016760 3367_ $$2ORCID$$aJOURNAL_ARTICLE
001016760 3367_ $$00$$2EndNote$$aJournal Article
001016760 520__ $$aThe combination of Li-metal anode and high-voltage cathode is regarded as a solution for the next-generation high-energy-density secondary batteries. However, a traditional electrolyte is either incompatible with the Li-metal anode or vulnerable to high voltage. This work reports a 1 M dual-salts Localized-High-Concentration-Electrolyte with Fluoroethylene carbonate (FEC) additive. It enables stable cycling of Li||LiNi0.8Co0.1Mn0.1O2 (NMC811) battery, which shows 81.5% capacity retention after 300 cycles with a charge/discharge current density of 1 C and a voltage range of 2.7–4.4 V. Scanning electron microscopy (SEM) images show that this electrolyte not only largely reduced Li dendrites and ‘dead’ Li on anode surface but also well protected the microstructure of NMC811 cathode. Possible components of both solid-electrolyte interlayer (SEI) and cathode-electrolyte interlayer (CEI) were characterized by energy-dispersive X-ray spectroscopy (EDX). The result illustrates that FEC protected Li salts from decomposition on the anode side and suppressed the decomposition of solvents on the cathode side.
001016760 536__ $$0G:(DE-HGF)POF4-1223$$a1223 - Batteries in Application (POF4-122)$$cPOF4-122$$fPOF IV$$x0
001016760 588__ $$aDataset connected to CrossRef, Journals: juser.fz-juelich.de
001016760 7001_ $$0P:(DE-Juel1)164875$$aWu, Baolin$$b1$$ufzj
001016760 7001_ $$0P:(DE-Juel1)173719$$aDanilov, Dmitri L.$$b2$$ufzj
001016760 7001_ $$0P:(DE-Juel1)156123$$aEichel, Rüdiger-A.$$b3$$ufzj
001016760 7001_ $$0P:(DE-Juel1)165918$$aNotten, Peter H. L.$$b4$$eCorresponding author
001016760 773__ $$0PERI:(DE-600)2813972-0$$a10.3390/batteries9090477$$gVol. 9, no. 9, p. 477 -$$n9$$p477 -$$tBatteries$$v9$$x2313-0105$$y2023
001016760 8564_ $$uhttps://juser.fz-juelich.de/record/1016760/files/batteries-09-00477.pdf$$yOpenAccess
001016760 8767_ $$d2023-10-09$$eAPC$$jZahlung erfolgt
001016760 909CO $$ooai:juser.fz-juelich.de:1016760$$pdnbdelivery$$popenCost$$pVDB$$pdriver$$pOpenAPC$$popen_access$$popenaire
001016760 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)190219$$aForschungszentrum Jülich$$b0$$kFZJ
001016760 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)164875$$aForschungszentrum Jülich$$b1$$kFZJ
001016760 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)173719$$aForschungszentrum Jülich$$b2$$kFZJ
001016760 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)156123$$aForschungszentrum Jülich$$b3$$kFZJ
001016760 9101_ $$0I:(DE-588b)36225-6$$6P:(DE-Juel1)156123$$aRWTH Aachen$$b3$$kRWTH
001016760 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)165918$$aForschungszentrum Jülich$$b4$$kFZJ
001016760 9131_ $$0G:(DE-HGF)POF4-122$$1G:(DE-HGF)POF4-120$$2G:(DE-HGF)POF4-100$$3G:(DE-HGF)POF4$$4G:(DE-HGF)POF$$9G:(DE-HGF)POF4-1223$$aDE-HGF$$bForschungsbereich Energie$$lMaterialien und Technologien für die Energiewende (MTET)$$vElektrochemische Energiespeicherung$$x0
001016760 9141_ $$y2023
001016760 915pc $$0PC:(DE-HGF)0000$$2APC$$aAPC keys set
001016760 915pc $$0PC:(DE-HGF)0003$$2APC$$aDOAJ Journal
001016760 915__ $$0StatID:(DE-HGF)0160$$2StatID$$aDBCoverage$$bEssential Science Indicators$$d2023-08-31
001016760 915__ $$0LIC:(DE-HGF)CCBY4$$2HGFVOC$$aCreative Commons Attribution CC BY 4.0
001016760 915__ $$0StatID:(DE-HGF)0501$$2StatID$$aDBCoverage$$bDOAJ Seal$$d2023-04-12T14:55:26Z
001016760 915__ $$0StatID:(DE-HGF)0500$$2StatID$$aDBCoverage$$bDOAJ$$d2023-04-12T14:55:26Z
001016760 915__ $$0StatID:(DE-HGF)0113$$2StatID$$aWoS$$bScience Citation Index Expanded$$d2023-08-31
001016760 915__ $$0StatID:(DE-HGF)0700$$2StatID$$aFees$$d2023-08-31
001016760 915__ $$0StatID:(DE-HGF)0510$$2StatID$$aOpenAccess
001016760 915__ $$0StatID:(DE-HGF)0030$$2StatID$$aPeer Review$$bDOAJ : Anonymous peer review$$d2023-04-12T14:55:26Z
001016760 915__ $$0StatID:(DE-HGF)0561$$2StatID$$aArticle Processing Charges$$d2023-08-31
001016760 915__ $$0StatID:(DE-HGF)0100$$2StatID$$aJCR$$bBATTERIES-BASEL : 2022$$d2023-10-26
001016760 915__ $$0StatID:(DE-HGF)0200$$2StatID$$aDBCoverage$$bSCOPUS$$d2023-10-26
001016760 915__ $$0StatID:(DE-HGF)0300$$2StatID$$aDBCoverage$$bMedline$$d2023-10-26
001016760 915__ $$0StatID:(DE-HGF)0199$$2StatID$$aDBCoverage$$bClarivate Analytics Master Journal List$$d2023-10-26
001016760 915__ $$0StatID:(DE-HGF)0150$$2StatID$$aDBCoverage$$bWeb of Science Core Collection$$d2023-10-26
001016760 915__ $$0StatID:(DE-HGF)1160$$2StatID$$aDBCoverage$$bCurrent Contents - Engineering, Computing and Technology$$d2023-10-26
001016760 915__ $$0StatID:(DE-HGF)1150$$2StatID$$aDBCoverage$$bCurrent Contents - Physical, Chemical and Earth Sciences$$d2023-10-26
001016760 915__ $$0StatID:(DE-HGF)9900$$2StatID$$aIF < 5$$d2023-10-26
001016760 920__ $$lyes
001016760 9201_ $$0I:(DE-Juel1)IEK-9-20110218$$kIEK-9$$lGrundlagen der Elektrochemie$$x0
001016760 9801_ $$aAPC
001016760 9801_ $$aFullTexts
001016760 980__ $$ajournal
001016760 980__ $$aVDB
001016760 980__ $$aUNRESTRICTED
001016760 980__ $$aI:(DE-Juel1)IEK-9-20110218
001016760 980__ $$aAPC
001016760 981__ $$aI:(DE-Juel1)IET-1-20110218