001024886 001__ 1024886
001024886 005__ 20250203103201.0
001024886 0247_ $$2doi$$a10.3390/batteries9050245
001024886 0247_ $$2datacite_doi$$a10.34734/FZJ-2024-02537
001024886 0247_ $$2WOS$$aWOS:000995544700001
001024886 037__ $$aFZJ-2024-02537
001024886 082__ $$a530
001024886 1001_ $$0P:(DE-Juel1)164794$$aReissig, Friederike$$b0
001024886 245__ $$aThe Role of Protective Surface Coatings on the Thermal Stability of Delithiated Ni-Rich Layered Oxide Cathode Materials
001024886 260__ $$aBasel$$bMDPI$$c2023
001024886 3367_ $$2DRIVER$$aarticle
001024886 3367_ $$2DataCite$$aOutput Types/Journal article
001024886 3367_ $$0PUB:(DE-HGF)16$$2PUB:(DE-HGF)$$aJournal Article$$bjournal$$mjournal$$s1712732992_15405
001024886 3367_ $$2BibTeX$$aARTICLE
001024886 3367_ $$2ORCID$$aJOURNAL_ARTICLE
001024886 3367_ $$00$$2EndNote$$aJournal Article
001024886 520__ $$aTo achieve a broader public acceptance for electric vehicles based on lithium-ion battery (LIB) technology, long driving ranges, low cost, and high safety are needed. A promising pathway to address these key parameters lies in the further improvement of Ni-rich cathode materials for LIB cells. Despite the higher achieved capacities and thus energy densities, there are major drawbacks in terms of capacity retention and thermal stability (of the charged cathode) which are crucial for customer acceptance and can be mitigated by protecting cathode particles. We studied the impact of surface modifications on cycle life and thermal stability of LiNi0.90Co0.05Mn0.05O2 layered oxide cathodes with WO3 by a simple sol–gel coating process. Several advanced analytical techniques such as low-energy ion scattering, differential scanning calorimetry, and high-temperature synchrotron X-ray powder diffraction of delithiated cathode materials, as well as charge/discharge cycling give significant insights into the impact of surface coverage of the coatings on mitigating degradation mechanisms. The results show that successful surface modifications of WO3 with a surface coverage of only 20% can prolong the cycle life of an LIB cell and play a crucial role in improving the thermal stability and, hence, the safety of LIBs.
001024886 536__ $$0G:(DE-HGF)POF4-1221$$a1221 - Fundamentals and Materials (POF4-122)$$cPOF4-122$$fPOF IV$$x0
001024886 588__ $$aDataset connected to CrossRef, Journals: juser.fz-juelich.de
001024886 7001_ $$00000-0002-1184-0756$$aRamirez-Rico, Joaquin$$b1
001024886 7001_ $$00000-0002-2097-5193$$aPlacke, Tobias Johannes$$b2
001024886 7001_ $$0P:(DE-Juel1)166130$$aWinter, Martin$$b3$$ufzj
001024886 7001_ $$00000-0002-5670-0327$$aSchmuch, Richard$$b4
001024886 7001_ $$00000-0001-7053-3986$$aGomez-Martin, Aurora$$b5$$eCorresponding author
001024886 773__ $$0PERI:(DE-600)2813972-0$$a10.3390/batteries9050245$$gVol. 9, no. 5, p. 245 -$$n5$$p245 -$$tBatteries$$v9$$x2313-0105$$y2023
001024886 8564_ $$uhttps://juser.fz-juelich.de/record/1024886/files/batteries-09-00245-v2.pdf$$yOpenAccess
001024886 8564_ $$uhttps://juser.fz-juelich.de/record/1024886/files/batteries-09-00245-v2.gif?subformat=icon$$xicon$$yOpenAccess
001024886 8564_ $$uhttps://juser.fz-juelich.de/record/1024886/files/batteries-09-00245-v2.jpg?subformat=icon-1440$$xicon-1440$$yOpenAccess
001024886 8564_ $$uhttps://juser.fz-juelich.de/record/1024886/files/batteries-09-00245-v2.jpg?subformat=icon-180$$xicon-180$$yOpenAccess
001024886 8564_ $$uhttps://juser.fz-juelich.de/record/1024886/files/batteries-09-00245-v2.jpg?subformat=icon-640$$xicon-640$$yOpenAccess
001024886 909CO $$ooai:juser.fz-juelich.de:1024886$$pdnbdelivery$$pdriver$$pVDB$$popen_access$$popenaire
001024886 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)166130$$aForschungszentrum Jülich$$b3$$kFZJ
001024886 9131_ $$0G:(DE-HGF)POF4-122$$1G:(DE-HGF)POF4-120$$2G:(DE-HGF)POF4-100$$3G:(DE-HGF)POF4$$4G:(DE-HGF)POF$$9G:(DE-HGF)POF4-1221$$aDE-HGF$$bForschungsbereich Energie$$lMaterialien und Technologien für die Energiewende (MTET)$$vElektrochemische Energiespeicherung$$x0
001024886 9141_ $$y2024
001024886 915__ $$0StatID:(DE-HGF)0200$$2StatID$$aDBCoverage$$bSCOPUS$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)0160$$2StatID$$aDBCoverage$$bEssential Science Indicators$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)1160$$2StatID$$aDBCoverage$$bCurrent Contents - Engineering, Computing and Technology$$d2023-10-26
001024886 915__ $$0LIC:(DE-HGF)CCBY4$$2HGFVOC$$aCreative Commons Attribution CC BY 4.0
001024886 915__ $$0StatID:(DE-HGF)0100$$2StatID$$aJCR$$bBATTERIES-BASEL : 2022$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)0501$$2StatID$$aDBCoverage$$bDOAJ Seal$$d2023-04-12T14:55:26Z
001024886 915__ $$0StatID:(DE-HGF)0500$$2StatID$$aDBCoverage$$bDOAJ$$d2023-04-12T14:55:26Z
001024886 915__ $$0StatID:(DE-HGF)0113$$2StatID$$aWoS$$bScience Citation Index Expanded$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)0700$$2StatID$$aFees$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)0150$$2StatID$$aDBCoverage$$bWeb of Science Core Collection$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)9900$$2StatID$$aIF < 5$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)0510$$2StatID$$aOpenAccess
001024886 915__ $$0StatID:(DE-HGF)0030$$2StatID$$aPeer Review$$bDOAJ : Anonymous peer review$$d2023-04-12T14:55:26Z
001024886 915__ $$0StatID:(DE-HGF)0561$$2StatID$$aArticle Processing Charges$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)1150$$2StatID$$aDBCoverage$$bCurrent Contents - Physical, Chemical and Earth Sciences$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)0300$$2StatID$$aDBCoverage$$bMedline$$d2023-10-26
001024886 915__ $$0StatID:(DE-HGF)0199$$2StatID$$aDBCoverage$$bClarivate Analytics Master Journal List$$d2023-10-26
001024886 9201_ $$0I:(DE-Juel1)IEK-12-20141217$$kIEK-12$$lHelmholtz-Institut Münster Ionenleiter für Energiespeicher$$x0
001024886 9801_ $$aFullTexts
001024886 980__ $$ajournal
001024886 980__ $$aVDB
001024886 980__ $$aUNRESTRICTED
001024886 980__ $$aI:(DE-Juel1)IEK-12-20141217
001024886 981__ $$aI:(DE-Juel1)IMD-4-20141217