001030117 1001_ $$0P:(DE-HGF)0$$aGnutzmann, Maike Michelle$$b0
001030117 245__ $$aDirect Recycling at the Material Level: Unravelling Challenges and Opportunities through a Case Study on Spent Ni‐Rich Layered Oxide‐Based Cathodes
001030117 260__ $$aWeinheim$$bWiley-VCH$$c2024
001030117 3367_ $$2DRIVER$$aarticle
001030117 3367_ $$2DataCite$$aOutput Types/Journal article
001030117 3367_ $$0PUB:(DE-HGF)16$$2PUB:(DE-HGF)$$aJournal Article$$bjournal$$mjournal$$s1727857636_6319
001030117 3367_ $$2BibTeX$$aARTICLE
001030117 3367_ $$2ORCID$$aJOURNAL_ARTICLE
001030117 3367_ $$00$$2EndNote$$aJournal Article
001030117 520__ $$aDirect recycling is a key technology for enabling a circular economy of spent lithium ion batteries (LIBs). For cathode active materials (CAMs), it is regarded as the tightest closed-loop and most efficient approach among current recycling techniques as it simply proceeds via re-lithiation and reconstruction of aged CAMs instead of separating them into elemental components. In this work, spent, i.e., morphologically and structurally decomposed CAM based on LiNi0.83Co0.12Mn0.05O2 (NCM-831205) is restored by mimicking conditions of original CAM synthesis. After evaluating and optimizing the high-temperature duration for CAM restoration and subsequent washing procedure, the recycled CAM is shown to maintain poly-crystallinity and tap density, successfully recover specific surface area, lithium content, crystal structure in surface and bulk, while, however, only partly the original secondary particle size and shape. Though, comparable in initial 100 charge/discharge cycles with pristine CAM in lithium ion-cells, the subsequent increase in resistance and capacity fading remains a challenge. High temperature during recycling can be regarded as a key challenge on material level, as it not only promotes detrimental surface carbonate species from residual carbon black but also enhances cation disorder and micro-/nanoscopic porosity through oxygen release, likely in de-lithiated, thus less thermally stable regions of cycled NCM.
001030117 536__ $$0G:(DE-HGF)POF4-1221$$a1221 - Fundamentals and Materials (POF4-122)$$cPOF4-122$$fPOF IV$$x0
001030117 536__ $$0G:(GEPRIS)459785385$$aDFG project G:(GEPRIS)459785385 - Röntgenpulverdiffraktometer (459785385)$$c459785385$$x1
001030117 588__ $$aDataset connected to DataCite
001030117 7001_ $$0P:(DE-HGF)0$$aMakvandi, Ardavan$$b1
001030117 7001_ $$0P:(DE-HGF)0$$aYing, Bixian$$b2
001030117 7001_ $$0P:(DE-HGF)0$$aBuchmann, Julius$$b3
001030117 7001_ $$0P:(DE-HGF)0$$aLüther, Marco Joes$$b4
001030117 7001_ $$0P:(DE-HGF)0$$aHelm, Bianca$$b5
001030117 7001_ $$0P:(DE-HGF)0$$aNagel, Peter$$b6
001030117 7001_ $$0P:(DE-HGF)0$$aPeterlechner, Martin$$b7
001030117 7001_ $$aWilde, Gerhard$$b8
001030117 7001_ $$0P:(DE-HGF)0$$aGomez-Martin, Aurora$$b9
001030117 7001_ $$0P:(DE-HGF)0$$aKleiner, Karin$$b10
001030117 7001_ $$0P:(DE-Juel1)166130$$aWinter, Martin$$b11
001030117 7001_ $$0P:(DE-Juel1)171865$$aKasnatscheew, Johannes$$b12
001030117 773__ $$0PERI:(DE-600)2594556-7$$a10.1002/aenm.202400840$$gp. 2400840$$n36$$p2400840$$tAdvanced energy materials$$v14$$x1614-6832$$y2024
001030117 8564_ $$uhttps://juser.fz-juelich.de/record/1030117/files/Advanced%20Energy%20Materials%20-%202024%20-%20Gnutzmann%20-%20Direct%20Recycling%20at%20the%20Material%20Level%20Unravelling%20Challenges%20and-1.pdf$$yOpenAccess
001030117 8564_ $$uhttps://juser.fz-juelich.de/record/1030117/files/Advanced%20Energy%20Materials%20-%202024%20-%20Gnutzmann%20-%20Direct%20Recycling%20at%20the%20Material%20Level%20Unravelling%20Challenges%20and-1.gif?subformat=icon$$xicon$$yOpenAccess
001030117 8564_ $$uhttps://juser.fz-juelich.de/record/1030117/files/Advanced%20Energy%20Materials%20-%202024%20-%20Gnutzmann%20-%20Direct%20Recycling%20at%20the%20Material%20Level%20Unravelling%20Challenges%20and-1.jpg?subformat=icon-1440$$xicon-1440$$yOpenAccess
001030117 8564_ $$uhttps://juser.fz-juelich.de/record/1030117/files/Advanced%20Energy%20Materials%20-%202024%20-%20Gnutzmann%20-%20Direct%20Recycling%20at%20the%20Material%20Level%20Unravelling%20Challenges%20and-1.jpg?subformat=icon-180$$xicon-180$$yOpenAccess
001030117 8564_ $$uhttps://juser.fz-juelich.de/record/1030117/files/Advanced%20Energy%20Materials%20-%202024%20-%20Gnutzmann%20-%20Direct%20Recycling%20at%20the%20Material%20Level%20Unravelling%20Challenges%20and-1.jpg?subformat=icon-640$$xicon-640$$yOpenAccess
001030117 909CO $$ooai:juser.fz-juelich.de:1030117$$pdnbdelivery$$pdriver$$pVDB$$popen_access$$popenaire
001030117 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)166130$$aForschungszentrum Jülich$$b11$$kFZJ
001030117 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)171865$$aForschungszentrum Jülich$$b12$$kFZJ
001030117 9131_ $$0G:(DE-HGF)POF4-122$$1G:(DE-HGF)POF4-120$$2G:(DE-HGF)POF4-100$$3G:(DE-HGF)POF4$$4G:(DE-HGF)POF$$9G:(DE-HGF)POF4-1221$$aDE-HGF$$bForschungsbereich Energie$$lMaterialien und Technologien für die Energiewende (MTET)$$vElektrochemische Energiespeicherung$$x0
001030117 9141_ $$y2024
001030117 915__ $$0StatID:(DE-HGF)0160$$2StatID$$aDBCoverage$$bEssential Science Indicators$$d2023-10-26
001030117 915__ $$0LIC:(DE-HGF)CCBY4$$2HGFVOC$$aCreative Commons Attribution CC BY 4.0
001030117 915__ $$0StatID:(DE-HGF)3001$$2StatID$$aDEAL Wiley$$d2023-10-26$$wger
001030117 915__ $$0StatID:(DE-HGF)0113$$2StatID$$aWoS$$bScience Citation Index Expanded$$d2023-10-26
001030117 915__ $$0StatID:(DE-HGF)0510$$2StatID$$aOpenAccess
001030117 915__ $$0StatID:(DE-HGF)0200$$2StatID$$aDBCoverage$$bSCOPUS$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)0300$$2StatID$$aDBCoverage$$bMedline$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)0199$$2StatID$$aDBCoverage$$bClarivate Analytics Master Journal List$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)1150$$2StatID$$aDBCoverage$$bCurrent Contents - Physical, Chemical and Earth Sciences$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)1160$$2StatID$$aDBCoverage$$bCurrent Contents - Engineering, Computing and Technology$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)0150$$2StatID$$aDBCoverage$$bWeb of Science Core Collection$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)0100$$2StatID$$aJCR$$bADV ENERGY MATER : 2022$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)0600$$2StatID$$aDBCoverage$$bEbsco Academic Search$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)0030$$2StatID$$aPeer Review$$bASC$$d2024-12-12
001030117 915__ $$0StatID:(DE-HGF)9925$$2StatID$$aIF >= 25$$bADV ENERGY MATER : 2022$$d2024-12-12
001030117 9201_ $$0I:(DE-Juel1)IMD-4-20141217$$kIMD-4$$lHelmholtz-Institut Münster Ionenleiter für Energiespeicher$$x0
001030117 980__ $$ajournal
001030117 980__ $$aVDB
001030117 980__ $$aUNRESTRICTED
001030117 980__ $$aI:(DE-Juel1)IMD-4-20141217
001030117 9801_ $$aFullTexts