000010831 001__ 10831
000010831 005__ 20240708132735.0
000010831 037__ $$aPreJuSER-10831
000010831 1001_ $$0P:(DE-HGF)0$$aKornely, M.$$b0
000010831 1112_ $$cLucerne, Switzerland$$d2010-06-29
000010831 245__ $$aDegradation of ASC performance by Cr-poisoning
000010831 260__ $$c2010
000010831 29510 $$a9th European Fuel Cell Forum
000010831 3367_ $$0PUB:(DE-HGF)6$$2PUB:(DE-HGF)$$aConference Presentation
000010831 3367_ $$033$$2EndNote$$aConference Paper
000010831 3367_ $$2DataCite$$aOther
000010831 3367_ $$2ORCID$$aLECTURE_SPEECH
000010831 3367_ $$2DRIVER$$aconferenceObject
000010831 3367_ $$2BibTeX$$aINPROCEEDINGS
000010831 500__ $$aRecord converted from VDB: 12.11.2012
000010831 500__ $$3Presentation on a conference
000010831 536__ $$0G:(DE-Juel1)FUEK402$$2G:(DE-HGF)$$aRationelle Energieumwandlung$$cP12$$x0
000010831 536__ $$0G:(DE-Juel1)SOFC-20140602$$aSOFC - Solid Oxide Fuel Cell (SOFC-20140602)$$cSOFC-20140602$$fSOFC$$x1
000010831 7001_ $$0P:(DE-Juel1)VDB98457$$aNeumann, A.$$b1$$uFZJ
000010831 7001_ $$0P:(DE-Juel1)129636$$aMenzler, N. H.$$b2$$uFZJ
000010831 7001_ $$0P:(DE-HGF)0$$aIvers-Tiffée, E.$$b3
000010831 909CO $$ooai:juser.fz-juelich.de:10831$$pVDB
000010831 9131_ $$0G:(DE-Juel1)FUEK402$$bEnergie$$kP12$$lRationelle Energieumwandlung$$vRationelle Energieumwandlung$$x0
000010831 9141_ $$y2010
000010831 9201_ $$0I:(DE-Juel1)VDB809$$d30.09.2010$$gIEF$$kIEF-1$$lWerkstoffsynthese und Herstellungsverfahren$$x0
000010831 970__ $$aVDB:(DE-Juel1)121417
000010831 980__ $$aVDB
000010831 980__ $$aConvertedRecord
000010831 980__ $$aconf
000010831 980__ $$aI:(DE-Juel1)IEK-1-20101013
000010831 980__ $$aUNRESTRICTED
000010831 981__ $$aI:(DE-Juel1)IMD-2-20101013
000010831 981__ $$aI:(DE-Juel1)IEK-1-20101013