000141349 001__ 141349
000141349 005__ 20240708132726.0
000141349 037__ $$aFZJ-2013-06533
000141349 1001_ $$0P:(DE-Juel1)156292$$aHammer, Eva-Maria$$b0$$eCorresponding author$$ufzj
000141349 1112_ $$aSol-Gel Konferenz$$cMadrid$$d2013-08-25 - 2013-08-30$$wSpain
000141349 245__ $$aSol-gel synthesis and lithium ion conductivity of Al(2)O(3)-substituted Li(7-3x)Al(x)La(3)Zr(2)O(12) as electrolyte for all-solid-state-Li-ion-batteries
000141349 260__ $$c2013
000141349 3367_ $$0PUB:(DE-HGF)17$$2PUB:(DE-HGF)$$aLecture$$blecture$$mlecture$$s1387355015_22436$$xOther
000141349 3367_ $$2DataCite$$aText
000141349 3367_ $$2BibTeX$$aMISC
000141349 3367_ $$2ORCID$$aLECTURE_SPEECH
000141349 3367_ $$031$$2EndNote$$aGeneric
000141349 3367_ $$2DRIVER$$alecture
000141349 536__ $$0G:(DE-HGF)POF2-123$$a123 - Fuel Cells (POF2-123)$$cPOF2-123$$fPOF II$$x0
000141349 7001_ $$0P:(DE-Juel1)129610$$aHan, Feng$$b1$$ufzj
000141349 7001_ $$0P:(DE-Juel1)129669$$aVan Gestel, Tim$$b2$$ufzj
000141349 7001_ $$0P:(DE-Juel1)129667$$aTietz, Frank$$b3$$ufzj
000141349 909CO $$ooai:juser.fz-juelich.de:141349$$pVDB
000141349 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)156292$$aForschungszentrum Jülich GmbH$$b0$$kFZJ
000141349 9101_ $$0I:(DE-HGF)0$$6P:(DE-Juel1)129610$$aExternal Institute$$b1$$kExtern
000141349 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)129669$$aForschungszentrum Jülich GmbH$$b2$$kFZJ
000141349 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)129667$$aForschungszentrum Jülich GmbH$$b3$$kFZJ
000141349 9131_ $$0G:(DE-HGF)POF2-123$$1G:(DE-HGF)POF2-120$$2G:(DE-HGF)POF2-100$$3G:(DE-HGF)POF2$$4G:(DE-HGF)POF$$aDE-HGF$$bEnergie$$lRationelle Energieumwandlung und -nutzung$$vFuel Cells$$x0
000141349 9141_ $$y2013
000141349 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$kIEK-1$$lWerkstoffsynthese und Herstellungsverfahren$$x0
000141349 980__ $$alecture
000141349 980__ $$aVDB
000141349 980__ $$aUNRESTRICTED
000141349 980__ $$aI:(DE-Juel1)IEK-1-20101013
000141349 981__ $$aI:(DE-Juel1)IMD-2-20101013