000015297 001__ 15297
000015297 005__ 20240708132657.0
000015297 037__ $$aPreJuSER-15297
000015297 1001_ $$0P:(DE-HGF)0$$aKornely, M.$$b0
000015297 1112_ $$cMontréal, Canada$$d2011-05-01
000015297 245__ $$aDegradation of solid oxide fuel cell performance by Cr-poisoning
000015297 260__ $$c2011
000015297 29510 $$aTwelfth International Symposium on Solid Oxide Fuel Cells (SOFC XII)
000015297 3367_ $$0PUB:(DE-HGF)6$$2PUB:(DE-HGF)$$aConference Presentation
000015297 3367_ $$033$$2EndNote$$aConference Paper
000015297 3367_ $$2DataCite$$aOther
000015297 3367_ $$2ORCID$$aLECTURE_SPEECH
000015297 3367_ $$2DRIVER$$aconferenceObject
000015297 3367_ $$2BibTeX$$aINPROCEEDINGS
000015297 500__ $$aRecord converted from VDB: 12.11.2012
000015297 500__ $$3Presentation on a conference
000015297 536__ $$0G:(DE-Juel1)FUEK402$$2G:(DE-HGF)$$aRationelle Energieumwandlung$$cP12$$x0
000015297 536__ $$0G:(DE-Juel1)SOFC-20140602$$aSOFC - Solid Oxide Fuel Cell (SOFC-20140602)$$cSOFC-20140602$$fSOFC$$x1
000015297 7001_ $$0P:(DE-Juel1)130388$$aNeumann, A.$$b1$$uFZJ
000015297 7001_ $$0P:(DE-Juel1)129636$$aMenzler, N.H.$$b2$$uFZJ
000015297 7001_ $$0P:(DE-HGF)0$$aWeber, A.$$b3
000015297 7001_ $$0P:(DE-HGF)0$$aIvers-Tiffée, E.$$b4
000015297 909CO $$ooai:juser.fz-juelich.de:15297$$pVDB
000015297 9131_ $$0G:(DE-Juel1)FUEK402$$bEnergie$$kP12$$lRationelle Energieumwandlung$$vRationelle Energieumwandlung$$x0
000015297 9141_ $$y2011
000015297 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$gIEK$$kIEK-1$$lWerkstoffsynthese und Herstellverfahren$$x0
000015297 970__ $$aVDB:(DE-Juel1)128088
000015297 980__ $$aVDB
000015297 980__ $$aConvertedRecord
000015297 980__ $$aconf
000015297 980__ $$aI:(DE-Juel1)IEK-1-20101013
000015297 980__ $$aUNRESTRICTED
000015297 981__ $$aI:(DE-Juel1)IMD-2-20101013