001     15819
005     20240711092258.0
024 7 _ |2 DOI
|a 10.1016/j.jpowsour.2011.02.086
024 7 _ |2 WOS
|a WOS:000290837000017
037 _ _ |a PreJuSER-15819
041 _ _ |a eng
082 _ _ |a 620
084 _ _ |2 WoS
|a Electrochemistry
084 _ _ |2 WoS
|a Energy & Fuels
100 1 _ |0 P:(DE-Juel1)129591
|a Bram, M.
|b 0
|u FZJ
245 _ _ |a Interaction of sealing material mica with interconnect steel for solid oxide fuel cells application at 600 degrees C
260 _ _ |a New York, NY [u.a.]
|b Elsevier
|c 2011
300 _ _ |a 5889 -5896
336 7 _ |a Journal Article
|0 PUB:(DE-HGF)16
|2 PUB:(DE-HGF)
336 7 _ |a Output Types/Journal article
|2 DataCite
336 7 _ |a Journal Article
|0 0
|2 EndNote
336 7 _ |a ARTICLE
|2 BibTeX
336 7 _ |a JOURNAL_ARTICLE
|2 ORCID
336 7 _ |a article
|2 DRIVER
440 _ 0 |0 3727
|a Journal of Power Sources
|v 196
|x 0378-7753
|y 14
500 _ _ |a The authors are grateful for financial support from the European Commission under contract No. SES6-2006-020089 (SOFC600). They also would like to thank B. Hausmann for manufacturing composite samples, V. Haanappel for conducting the experiments in the dual environment, M. Kappertz for helping in metallographic preparation, H. Moitroux for taking macro pictures and E. Wessel for SEM/EDX investigations. We would also like to thank W.J. Quadakkers for helpful discussions.
520 _ _ |a In the last few years, a lot of effort has been undertaken to reduce the operation temperature of solid oxide fuel cells (SOFCs). Intermediate temperatures in the range of 600-650 degrees C are thought to be highly attractive due to the expected reduction of high-temperature corrosion and interdiffusion phenomena. Furthermore, each stack operated at higher temperatures has to pass this temperature range during thermal cycling. In this work, a study has been carried out to investigate the interaction between interconnect steel (DIN 1.4760) and vermiculite mica paper filled with talc at 600 degrees C. Mica paper has been implemented recently as a new sealing material for SOFC stacks, aiming to replace established but brittle glass ceramics. Corrosion experiments were conducted at 600 degrees C under dual gas atmosphere conditions as well as in air. The interconnect steel showed the formation of non-protective oxide scales in contact with mica, especially in the presence of air. The morphology of oxide scales was investigated by SEM/EDX. Possible reasons for this unexpected result are discussed. The complete encapsulation of mica by embossed and welded sheets made of FeCrAlY-steel (DIN 1.4767) as well as the pre-oxidation of interconnect steel were investigated as solutions to this problem. Pre-oxidation was found to be a promising measure to protect the interconnect steel from breakaway oxidation in contact with mica. (C) 2011 Elsevier B.V. All rights reserved.
536 _ _ |0 G:(DE-Juel1)FUEK402
|2 G:(DE-HGF)
|a Rationelle Energieumwandlung
|c P12
|x 0
536 _ _ |0 G:(DE-Juel1)SOFC-20140602
|a SOFC - Solid Oxide Fuel Cell (SOFC-20140602)
|c SOFC-20140602
|f SOFC
|x 1
588 _ _ |a Dataset connected to Web of Science
650 _ 7 |2 WoSType
|a J
653 2 0 |2 Author
|a Sealing SOFC
653 2 0 |2 Author
|a Mica
653 2 0 |2 Author
|a Interconnect steel
653 2 0 |2 Author
|a Oxidation
653 2 0 |2 Author
|a Intermediate temperature
700 1 _ |0 P:(DE-Juel1)VDB2712
|a Niewolak, L.
|b 1
|u FZJ
700 1 _ |0 P:(DE-Juel1)VDB97509
|a Shah, N.
|b 2
|u FZJ
700 1 _ |0 P:(DE-Juel1)129662
|a Sebold, D.
|b 3
|u FZJ
700 1 _ |0 P:(DE-Juel1)129594
|a Buchkremer, H.P.
|b 4
|u FZJ
773 _ _ |0 PERI:(DE-600)1491915-1
|a 10.1016/j.jpowsour.2011.02.086
|g Vol. 196, p. 5889 -5896
|p 5889 -5896
|q 196<5889 -5896
|t Journal of power sources
|v 196
|x 0378-7753
|y 2011
856 7 _ |u http://dx.doi.org/10.1016/j.jpowsour.2011.02.086
856 4 _ |u https://juser.fz-juelich.de/record/15819/files/FZJ-15819_PV.pdf
|z Published final document.
|y Restricted
909 C O |o oai:juser.fz-juelich.de:15819
|p VDB
913 1 _ |0 G:(DE-Juel1)FUEK402
|a DE-HGF
|b Energie
|k P12
|l Rationelle Energieumwandlung
|v Rationelle Energieumwandlung
|x 0
913 2 _ |0 G:(DE-HGF)POF3-135
|1 G:(DE-HGF)POF3-130
|2 G:(DE-HGF)POF3-100
|a DE-HGF
|b Forschungsbereich Energie
|l Speicher und vernetzte Infrastrukturen
|v Fuel Cells
|x 0
914 1 _ |y 2011
915 _ _ |0 StatID:(DE-HGF)0010
|a JCR/ISI refereed
920 1 _ |0 I:(DE-Juel1)IEK-1-20101013
|g IEK
|k IEK-1
|l Werkstoffsynthese und Herstellverfahren
|x 0
920 1 _ |0 I:(DE-Juel1)IEK-2-20101013
|g IEK
|k IEK-2
|l Werkstoffstruktur und -eigenschaften
|x 1
970 _ _ |a VDB:(DE-Juel1)129150
980 _ _ |a VDB
980 _ _ |a ConvertedRecord
980 _ _ |a journal
980 _ _ |a I:(DE-Juel1)IEK-1-20101013
980 _ _ |a I:(DE-Juel1)IEK-2-20101013
980 _ _ |a UNRESTRICTED
981 _ _ |a I:(DE-Juel1)IMD-1-20101013
981 _ _ |a I:(DE-Juel1)IMD-2-20101013
981 _ _ |a I:(DE-Juel1)IEK-2-20101013


LibraryCollectionCLSMajorCLSMinorLanguageAuthor
Marc 21