000016150 001__ 16150
000016150 005__ 20240709094441.0
000016150 037__ $$aPreJuSER-16150
000016150 1001_ $$0P:(DE-Juel1)129819$$aZurek, J.$$b0$$uFZJ
000016150 1112_ $$cNew London, NH, USA$$d2011-07-24
000016150 245__ $$aScale formation and phase transformations during long term steam oxidation of the high-Cr austenitic steel SANICRO25 in the temperature range 600 - 750 °C
000016150 260__ $$c2011
000016150 29510 $$aGordon Rearch Conference High Temperature Corrosion
000016150 3367_ $$0PUB:(DE-HGF)24$$2PUB:(DE-HGF)$$aPoster
000016150 3367_ $$033$$2EndNote$$aConference Paper
000016150 3367_ $$2DataCite$$aOutput Types/Conference Poster
000016150 3367_ $$2DRIVER$$aconferenceObject
000016150 3367_ $$2ORCID$$aCONFERENCE_POSTER
000016150 3367_ $$2BibTeX$$aINPROCEEDINGS
000016150 500__ $$aRecord converted from VDB: 12.11.2012
000016150 536__ $$0G:(DE-Juel1)FUEK402$$2G:(DE-HGF)$$aRationelle Energieumwandlung$$cP12$$x0
000016150 7001_ $$0P:(DE-Juel1)129662$$aSebold, D.$$b1$$uFZJ
000016150 7001_ $$0P:(DE-Juel1)VDB72741$$aHüttel, T.$$b2$$uFZJ
000016150 7001_ $$0P:(DE-Juel1)129782$$aQuadakkers, W.J.$$b3$$uFZJ
000016150 909CO $$ooai:juser.fz-juelich.de:16150$$pVDB
000016150 9131_ $$0G:(DE-Juel1)FUEK402$$bEnergie$$kP12$$lRationelle Energieumwandlung$$vRationelle Energieumwandlung$$x0
000016150 9141_ $$y2011
000016150 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$gIEK$$kIEK-1$$lWerkstoffsynthese und Herstellverfahren$$x0
000016150 9201_ $$0I:(DE-Juel1)IEK-2-20101013$$gIEK$$kIEK-2$$lWerkstoffstruktur und -eigenschaften$$x1
000016150 970__ $$aVDB:(DE-Juel1)129850
000016150 980__ $$aVDB
000016150 980__ $$aConvertedRecord
000016150 980__ $$aposter
000016150 980__ $$aI:(DE-Juel1)IEK-1-20101013
000016150 980__ $$aI:(DE-Juel1)IEK-2-20101013
000016150 980__ $$aUNRESTRICTED
000016150 981__ $$aI:(DE-Juel1)IMD-1-20101013
000016150 981__ $$aI:(DE-Juel1)IMD-2-20101013
000016150 981__ $$aI:(DE-Juel1)IEK-2-20101013