000017520 001__ 17520
000017520 005__ 20240708132707.0
000017520 037__ $$aPreJuSER-17520
000017520 1001_ $$0P:(DE-Juel1)140203$$aEbert, S.$$b0$$uFZJ
000017520 1112_ $$cHamburg$$d2011-09-27
000017520 245__ $$aFailure mechanism of non-stoichiometric Mg-Al-Spinel abradable coatings under thermal cyclic loading
000017520 260__ $$c2011
000017520 29510 $$aInternational Thermal Spray Conference and Exposition 2011 (ITSC 2011)
000017520 3367_ $$0PUB:(DE-HGF)6$$2PUB:(DE-HGF)$$aConference Presentation
000017520 3367_ $$033$$2EndNote$$aConference Paper
000017520 3367_ $$2DataCite$$aOther
000017520 3367_ $$2ORCID$$aLECTURE_SPEECH
000017520 3367_ $$2DRIVER$$aconferenceObject
000017520 3367_ $$2BibTeX$$aINPROCEEDINGS
000017520 500__ $$aRecord converted from VDB: 12.11.2012
000017520 500__ $$3Presentation on a conference
000017520 536__ $$0G:(DE-Juel1)FUEK402$$2G:(DE-HGF)$$aRationelle Energieumwandlung$$cP12$$x0
000017520 7001_ $$0P:(DE-Juel1)VDB84038$$aSteinke, T.$$b1$$uFZJ
000017520 7001_ $$0P:(DE-Juel1)129670$$aVaßen, R.$$b2$$uFZJ
000017520 7001_ $$0P:(DE-Juel1)129666$$aStöver, D.$$b3$$uFZJ
000017520 909CO $$ooai:juser.fz-juelich.de:17520$$pVDB
000017520 9131_ $$0G:(DE-Juel1)FUEK402$$bEnergie$$kP12$$lRationelle Energieumwandlung$$vRationelle Energieumwandlung$$x0
000017520 9141_ $$y2011
000017520 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$gIEK$$kIEK-1$$lWerkstoffsynthese und Herstellverfahren$$x0
000017520 970__ $$aVDB:(DE-Juel1)132017
000017520 980__ $$aVDB
000017520 980__ $$aConvertedRecord
000017520 980__ $$aconf
000017520 980__ $$aI:(DE-Juel1)IEK-1-20101013
000017520 980__ $$aUNRESTRICTED
000017520 981__ $$aI:(DE-Juel1)IMD-2-20101013