000018360 245__ $$aScale Formation and Phase Transformations During Long Term Steam Oxidation of the High Cr Austenitic Steel SANICRO25 in the Temperature Range 600-750°C
000018360 260__ $$c2011
000018360 29510 $$aGordon Research Conference on "High Temperature Corrosion
000018360 3367_ $$0PUB:(DE-HGF)6$$2PUB:(DE-HGF)$$aConference Presentation
000018360 3367_ $$033$$2EndNote$$aConference Paper
000018360 3367_ $$2DataCite$$aOther
000018360 3367_ $$2ORCID$$aLECTURE_SPEECH
000018360 3367_ $$2DRIVER$$aconferenceObject
000018360 3367_ $$2BibTeX$$aINPROCEEDINGS
000018360 500__ $$aRecord converted from VDB: 12.11.2012
000018360 500__ $$3Presentation on a conference
000018360 536__ $$0G:(DE-Juel1)FUEK402$$2G:(DE-HGF)$$aRationelle Energieumwandlung$$cP12$$x0
000018360 7001_ $$0P:(DE-Juel1)129662$$aSebold, D.$$b1$$uFZJ
000018360 7001_ $$0P:(DE-Juel1)VDB72741$$aHüttel, T.$$b2$$uFZJ
000018360 7001_ $$0P:(DE-Juel1)129782$$aQuadakkers, W.J.$$b3$$uFZJ
000018360 909CO $$ooai:juser.fz-juelich.de:18360$$pVDB
000018360 9131_ $$0G:(DE-Juel1)FUEK402$$bEnergie$$kP12$$lRationelle Energieumwandlung$$vRationelle Energieumwandlung$$x0
000018360 9141_ $$y2011
000018360 9201_ $$0I:(DE-Juel1)IEK-2-20101013$$gIEK$$kIEK-2$$lWerkstoffstruktur und -eigenschaften$$x0
000018360 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$gIEK$$kIEK-1$$lWerkstoffsynthese und Herstellverfahren$$x1
000018360 970__ $$aVDB:(DE-Juel1)133025
000018360 980__ $$aVDB
000018360 980__ $$aConvertedRecord
000018360 980__ $$aconf
000018360 980__ $$aI:(DE-Juel1)IEK-2-20101013
000018360 980__ $$aI:(DE-Juel1)IEK-1-20101013
000018360 980__ $$aUNRESTRICTED
000018360 981__ $$aI:(DE-Juel1)IMD-1-20101013
000018360 981__ $$aI:(DE-Juel1)IMD-2-20101013
000018360 981__ $$aI:(DE-Juel1)IEK-1-20101013