% IMPORTANT: The following is UTF-8 encoded. This means that in the presence
% of non-ASCII characters, it will not work with BibTeX 0.99 or older.
% Instead, you should use an up-to-date BibTeX implementation like “bibtex8” or
% “biber”.
@ARTICLE{Ueda:186017,
author = {Ueda, Y. and Oya, M. and Hamaji, Y. and Lee, H. T. and
Kurishita, H. and Torikai, Y. and Yoshida, N. and Kreter, A.
and Coenen, J. W. and Litnovsky, A. and Philipps, V.},
title = {{S}urface erosion and modification of toughened,
fine-grained, recrystallized tungsten exposed to {TEXTOR}
edge plasma},
journal = {Physica scripta},
volume = {T159},
issn = {1402-4896},
address = {Bristol},
publisher = {IoP Publ.},
reportid = {FZJ-2015-00126},
pages = {014038},
year = {2014},
abstract = {In order to evaluate the applicability of toughened,
fine-grained, recrystallized (TFGR)-W to tokamak edge plasma
environment, two TFGR-W specimens (TFGR-W $1.1wt\%TiC$ and
TFGR-W $3.3wt\%TaC)$ were exposed to 31 identical ohmic
discharges in the TEXTOR tokamak by means of a limiter lock
system. The highest surface temperature reached was about
1300 °C. Under these temperature conditions, the bulk
microstructure and dispersoids distribution of both TFGR-W
remained intact, suggesting that these TFGR-W tungsten
materials have sufficient stability under these plasma
loading conditions. The erosion of TiC dispersoids on the
surface was enhanced by plasma exposure above 1150 °C,
while such enhanced erosion was not observed for TaC
dispersoids probably due to the higher melting temperature
of Ta than Ti.},
cin = {IEK-4},
ddc = {530},
cid = {I:(DE-Juel1)IEK-4-20101013},
pnm = {135 - Plasma-wall interactions (POF2-135)},
pid = {G:(DE-HGF)POF2-135},
typ = {PUB:(DE-HGF)16},
UT = {WOS:000334847800039},
doi = {10.1088/0031-8949/2014/T159/014038},
url = {https://juser.fz-juelich.de/record/186017},
}