@ARTICLE{Grushko:201277,
author = {Grushko, Benjamin},
title = {{A}gain regarding the {A}l−{P}d phase diagram},
journal = {Journal of alloys and compounds},
volume = {557},
issn = {0925-8388},
address = {Lausanne},
publisher = {Elsevier},
reportid = {FZJ-2015-03582},
pages = {102 - 111},
year = {2013},
abstract = {The Al−Pd phase diagram was experimentally reinvestigated
in the region around the equiatomic composition. The
high-temperature β-phase (CsCl-type structure) forming
around AlPd transforms by cooling to a rhombohedral
β′-phase, which only being metastable, strongly resists
transformation to the stable low-temperature μ-phase
(FeSi-type structure). The composition of the β-phase
ranges between Al57.5Pd42.5 (at 949 °C) and Al45Pd55 (at
1315 °C). The highest existence temperature of the μ-phase
is 745 °C at ∼Al52Pd48. The reaction β ↔ μ + δ
occurs at 735 °C and Al53Pd47 composition; the reaction β
↔ μ + ν occurs (provisionally) at somewhat below 630 °C
and ∼Al48Pd52 composition. No eutectoid decomposition of
the ν-phase was observed down to 400 °C. A compositional
continuity of the high-temperature complex ε6 and ε28
phases is argued.},
cin = {PGI-5},
ddc = {670},
cid = {I:(DE-Juel1)PGI-5-20110106},
pnm = {424 - Exploratory materials and phenomena (POF2-424)},
pid = {G:(DE-HGF)POF2-424},
typ = {PUB:(DE-HGF)16},
UT = {WOS:000315185000018},
doi = {10.1016/j.jallcom.2012.12.145},
url = {https://juser.fz-juelich.de/record/201277},
}