@ARTICLE{Jeganathan:203124,
author = {Jeganathan, K. and Purushothaman, V. and Debnath, R. K. and
Calarco, R. and Luth, H.},
title = {{R}aman scattering on intrinsic surface electron
accumulation of {I}n{N} nanowires},
journal = {Applied physics letters},
volume = {97},
number = {9},
issn = {0003-6951},
address = {Melville, NY},
publisher = {American Inst. of Physics},
reportid = {FZJ-2015-05139},
pages = {093104 -},
year = {2010},
abstract = {An intrinsic property of vertically aligned InN nanowire
(NW) ensembles have been investigated by analysis of coupled
longitudinal optical (LO) phonon mode using μ-Raman
scattering. Spectra were recorded in backscattering
geometries in parallel and perpendicular to the axis of the
NWs. The width of surface accumulation layer is estimated
from the LO phonon peak intensity ratios. The carrier
concentration is extracted to be 6.7×1016 cm−3. The
pronounced peak at 627.2 cm−1 is related to the
interaction of phonons with surface electrons. The surface
charge density, Nsc is calculated to be
∼2.55×1013 cm−2 which provides surface accumulation
field strength of 5.5 Mv/cm.},
cin = {PGI-9},
ddc = {530},
cid = {I:(DE-Juel1)PGI-9-20110106},
pnm = {899 - ohne Topic (POF3-899)},
pid = {G:(DE-HGF)POF3-899},
typ = {PUB:(DE-HGF)16},
UT = {WOS:000282187200055},
doi = {10.1063/1.3483758},
url = {https://juser.fz-juelich.de/record/203124},
}