000021860 001__ 21860
000021860 005__ 20240708132707.0
000021860 037__ $$aPreJuSER-21860
000021860 1001_ $$0P:(DE-HGF)0$$aKornely, M.$$b0
000021860 1112_ $$cLucerne, Switzerland$$d2012-06-26
000021860 245__ $$aDegradation of high performance cathode by Cr-poisoning at OCV-conditions
000021860 260__ $$c2012
000021860 29510 $$a10th European SOFC Forum
000021860 3367_ $$0PUB:(DE-HGF)31$$2PUB:(DE-HGF)$$aTalk (non conference)
000021860 3367_ $$033$$2EndNote$$aConference Paper
000021860 3367_ $$2DataCite$$aOther
000021860 3367_ $$2DINI$$aOther
000021860 3367_ $$2BibTeX$$aINPROCEEDINGS
000021860 3367_ $$2ORCID$$aLECTURE_SPEECH
000021860 500__ $$aRecord converted from VDB: 12.11.2012
000021860 500__ $$3Talk (non conference)
000021860 536__ $$0G:(DE-Juel1)FUEK402$$2G:(DE-HGF)$$aRationelle Energieumwandlung$$cP12$$x0
000021860 536__ $$0G:(DE-Juel1)SOFC-20140602$$aSOFC - Solid Oxide Fuel Cell (SOFC-20140602)$$cSOFC-20140602$$fSOFC$$x1
000021860 7001_ $$0P:(DE-Juel1)129636$$aMenzler, N.H.$$b1$$uFZJ
000021860 7001_ $$0P:(DE-HGF)0$$aWeber, A.$$b2
000021860 7001_ $$0P:(DE-HGF)0$$aIvers-Tiffée, E.$$b3
000021860 909CO $$ooai:juser.fz-juelich.de:21860$$pVDB
000021860 9131_ $$0G:(DE-Juel1)FUEK402$$1G:(DE-HGF)POF2-120$$2G:(DE-HGF)POF2-100$$bEnergie$$kP12$$lRationelle Energieumwandlung$$vRationelle Energieumwandlung$$x0
000021860 9141_ $$y2012
000021860 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$gIEK$$kIEK-1$$lWerkstoffsynthese und Herstellverfahren$$x0
000021860 970__ $$aVDB:(DE-Juel1)138002
000021860 980__ $$aVDB
000021860 980__ $$aConvertedRecord
000021860 980__ $$atalk
000021860 980__ $$aI:(DE-Juel1)IEK-1-20101013
000021860 980__ $$aUNRESTRICTED
000021860 981__ $$aI:(DE-Juel1)IMD-2-20101013