000023009 001__ 23009
000023009 005__ 20240711085611.0
000023009 0247_ $$2DOI$$a10.1016/j.jpowsour.2012.09.061
000023009 0247_ $$2WOS$$aWOS:000312426700021
000023009 037__ $$aPreJuSER-23009
000023009 082__ $$a620
000023009 1001_ $$0P:(DE-Juel1)129667$$aTietz, F.$$b0$$uFZJ
000023009 245__ $$aDegradation phenomena in a solid oxide electrolysis cell after 9000 hours of operation
000023009 260__ $$aNew York, NY [u.a.]$$bElsevier$$c2013
000023009 300__ $$a129 - 135
000023009 3367_ $$0PUB:(DE-HGF)16$$2PUB:(DE-HGF)$$aJournal Article
000023009 3367_ $$2DataCite$$aOutput Types/Journal article
000023009 3367_ $$00$$2EndNote$$aJournal Article
000023009 3367_ $$2BibTeX$$aARTICLE
000023009 3367_ $$2ORCID$$aJOURNAL_ARTICLE
000023009 3367_ $$2DRIVER$$aarticle
000023009 440_0 $$03727$$aJournal of Power Sources$$v223$$x0378-7753
000023009 500__ $$3POF3_Assignment on 2016-02-29
000023009 500__ $$aRecord converted from VDB: 12.11.2012
000023009 536__ $$0G:(DE-Juel1)FUEK402$$2G:(DE-HGF)$$aRationelle Energieumwandlung$$cP12$$x0
000023009 536__ $$0G:(DE-Juel1)SOFC-20140602$$aSOFC - Solid Oxide Fuel Cell (SOFC-20140602)$$cSOFC-20140602$$fSOFC$$x1
000023009 7001_ $$0P:(DE-Juel1)129662$$aSebold, D.$$b1$$uFZJ
000023009 7001_ $$0P:(DE-HGF)0$$aBrisse, A$$b2
000023009 7001_ $$0P:(DE-HGF)0$$aSchefold, J.$$b3
000023009 773__ $$0PERI:(DE-600)1491915-1$$a10.1016/j.jpowsour.2012.09.061$$gVol. 223, p. 129 - 135$$p129 - 135$$q223<129 - 135$$tJournal of power sources$$v223$$x0378-7753$$y2013
000023009 8567_ $$uhttp://dx.doi.org/10.1016/j.jpowsour.2012.09.061
000023009 8564_ $$uhttps://juser.fz-juelich.de/record/23009/files/FZJ-23009.pdf$$yRestricted$$zPublished final document.
000023009 909CO $$ooai:juser.fz-juelich.de:23009$$pVDB
000023009 9131_ $$0G:(DE-Juel1)FUEK402$$bEnergie$$kP12$$lRationelle Energieumwandlung$$vRationelle Energieumwandlung$$x0
000023009 9132_ $$0G:(DE-HGF)POF3-139H$$1G:(DE-HGF)POF3-130$$2G:(DE-HGF)POF3-100$$aDE-HGF$$bForschungsbereich Energie$$lSpeicher und vernetzte Infrastrukturen$$vAddenda$$x0
000023009 9141_ $$y2013
000023009 915__ $$0StatID:(DE-HGF)0010$$aJCR/ISI refereed
000023009 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$gIEK$$kIEK-1$$lWerkstoffsynthese und Herstellverfahren$$x0
000023009 970__ $$aVDB:(DE-Juel1)139895
000023009 980__ $$aVDB
000023009 980__ $$aConvertedRecord
000023009 980__ $$ajournal
000023009 980__ $$aI:(DE-Juel1)IEK-1-20101013
000023009 980__ $$aUNRESTRICTED
000023009 981__ $$aI:(DE-Juel1)IMD-2-20101013