245 _ _ |a Effect of In-Situ Gas Changes on ThermallyGrown Chromia Scales Formed on Ni-25Cr Alloy at 1000°C in Atmospheres With and Without Water Vapour
260 _ _ |a Amsterdam [u.a.]
|c 2015
|b Elsevier Science
336 7 _ |a Journal Article
|b journal
|m journal
|0 PUB:(DE-HGF)16
|s 1449824366_10435
|2 PUB:(DE-HGF)
336 7 _ |a Output Types/Journal article
|2 DataCite
336 7 _ |a Journal Article
|0 0
|2 EndNote
336 7 _ |a ARTICLE
|2 BibTeX
336 7 _ |a JOURNAL_ARTICLE
|2 ORCID
336 7 _ |a article
|2 DRIVER
520 _ _ |a Regarding oxidation resistance, most high temperature alloys rely on the formation of a protective chromia surface scale during service. In the present study, the oxidation behaviour of a Ni–25%Cr model alloy was investigated during single- and two-stage oxidation in Ar–O2 and Ar–H2O gas mixtures at 1000°C. In the two-stage experiments, the test gas was changed after a predefined oxidation time from dry to wet gas, and vice versa, without intermediate specimen cooling. Oxidation kinetics were measured using thermogravimetry and post exposure characterisation was accomplished using scanning and transmission electron microscopy, focused ion beam and energy dispersive X-ray spectroscopy techniques. The single stage exposure to Ar–O2 resulted in the formation of a voided, poorly adhering chromia scale exhibiting a coarse, equi-axed morphology. In Ar–7%H2O a fine, columnar grained oxide scale was formed which was free of microvoidage within the scale and at the scale/metal interface and therefore exhibited excellent adherence to the metallic substrate. During two-stage exposure to Ar–O2 and subsequently to Ar–H2O, a fine grained, columnar shaped oxide developed on top of the coarse oxide scale formed in the first oxidation stage. The opposite effect occurred when the exposure started in the wet environment. The mechanisms which are responsible for the observed oxidation features are discussed on the basis of classical oxidation theory in combination with previous results on oxidation of chromia forming alloys in oxygen rich gases and water vapour containing, low p(O2) environments.
536 _ _ |a 111 - Efficient and Flexible Power Plants (POF3-111)
|0 G:(DE-HGF)POF3-111
|c POF3-111
|f POF III
|x 0
700 1 _ |a Gorr, B.
|0 P:(DE-HGF)0
|b 1
700 1 _ |a Hänsel, Michael
|0 P:(DE-Juel1)129729
|b 2
700 1 _ |a Shemet, Vladimir
|0 P:(DE-Juel1)129794
|b 3
700 1 _ |a Christ, H. J.
|0 P:(DE-HGF)0
|b 4
700 1 _ |a Quadakkers, Willem J.
|0 P:(DE-Juel1)129782
|b 5
773 _ _ |a 10.1179/0960340914Z.000000000108
|0 PERI:(DE-600)2035150-1
|n 1-2
|p 238-247
|t Materials at high temperatures
|v 32
|y 2015
|x 0960-3409
909 C O |o oai:juser.fz-juelich.de:279585
|p VDB
910 1 _ |a Forschungszentrum Jülich GmbH
|0 I:(DE-588b)5008462-8
|k FZJ
|b 2
|6 P:(DE-Juel1)129729
910 1 _ |a Forschungszentrum Jülich GmbH
|0 I:(DE-588b)5008462-8
|k FZJ
|b 3
|6 P:(DE-Juel1)129794
910 1 _ |a Forschungszentrum Jülich GmbH
|0 I:(DE-588b)5008462-8
|k FZJ
|b 5
|6 P:(DE-Juel1)129782
913 1 _ |a DE-HGF
|l Energieeffizienz, Materialien und Ressourcen
|1 G:(DE-HGF)POF3-110
|0 G:(DE-HGF)POF3-111
|2 G:(DE-HGF)POF3-100
|v Efficient and Flexible Power Plants
|x 0
|4 G:(DE-HGF)POF
|3 G:(DE-HGF)POF3
|b Energie
914 1 _ |y 2015
915 _ _ |a JCR
|0 StatID:(DE-HGF)0100
|2 StatID
|b MATER HIGH TEMP : 2014
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0200
|2 StatID
|b SCOPUS
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0199
|2 StatID
|b Thomson Reuters Master Journal List
915 _ _ |a WoS
|0 StatID:(DE-HGF)0111
|2 StatID
|b Science Citation Index Expanded
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0150
|2 StatID
|b Web of Science Core Collection
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)1160
|2 StatID
|b Current Contents - Engineering, Computing and Technology
915 _ _ |a IF < 5
|0 StatID:(DE-HGF)9900
|2 StatID
920 1 _ |0 I:(DE-Juel1)IEK-2-20101013
|k IEK-2
|l Werkstoffstruktur und -eigenschaften
|x 0
980 _ _ |a journal
980 _ _ |a VDB
980 _ _ |a I:(DE-Juel1)IEK-2-20101013
980 _ _ |a UNRESTRICTED
981 _ _ |a I:(DE-Juel1)IMD-1-20101013


LibraryCollectionCLSMajorCLSMinorLanguageAuthor
Marc 21