      title        = {{S}imulation calculations of mutual contamination between
                      tungsten and carbon and its impact on plasma surface
                      interactions},
      journal      = {Journal of nuclear materials},
      volume       = {290-293},
      issn         = {0022-3115},
      address      = {Amsterdam [u.a.]},
      publisher    = {Elsevier Science},
      reportid     = {PreJuSER-37926},
      pages        = {303 - 307},
      year         = {2001},
      note         = {Record converted from VDB: 12.11.2012},
      abstract     = {Mutual contamination between C and W, resulting from the
                      simultaneous use of these materials as plasma facing
                      components, is simulated by means of a computer simulation
                      code, Erosion and Deposition based on Dynamic model (EDDY).
                      W deposition on C rapidly increases the reflection
                      coefficient for D and C impurity. In comparison between the
                      calculation and a C-W twin test limiter experiment in
                      TEXTOR-94, C release from the C side of the limiter is
                      dominated by reflection of C impurity from the W deposits,
                      in addition to physical sputtering of C; chemical erosion is
                      strongly suppressed. Due to the dynamic effect which makes
                      C-W mixed layer, C deposition on W gradually changes the
                      reflection coefficient and sputter yields. Formation of a
                      sharp boundary between erosion and C deposition zones on the
                      W side of the limiter is well reproduced by simulation.
                      Local redeposition patterns of C and W on the limiter
                      surface are also calculated. (C) 2001 Elsevier Science B.V,
                      All rights reserved.},
      keywords     = {J (WoSType)},
      cin          = {IPP-1 / IPP-2},
      ddc          = {530},
      cid          = {I:(DE-Juel1)VDB27 / I:(DE-Juel1)VDB28},
      pnm          = {Wandkonditionierung und Plasma-Wand-Prozesse / Teilchen-
                      und Energietransport in der Plasmarandschicht /
                      Verunreinigungsquellen in Tokamaks},
      pid          = {G:(DE-Juel1)FUEK46 / G:(DE-Juel1)FUEK48 /
                      G:(DE-Juel1)FUEK47},
      shelfmark    = {Materials Science, Multidisciplinary / Nuclear Science $\&$
                      Technology / Mining $\&$ Mineral Processing},
      typ          = {PUB:(DE-HGF)16},
      UT           = {WOS:000167676700061},
      doi          = {10.1016/S0022-3115(00)00632-2},
      url          = {https://juser.fz-juelich.de/record/37926},
}