@ARTICLE{Pospieszczyk:37993,
      author       = {Pospieszczyk, A. and Tanabe, T. and Philipps, V. and
                      Sergienko, G. and Ohgo, T. and Kondo, K. and Wada, M. and
                      Rubel, M. and von Seggern, J. and Biel, W. and Huber, A. and
                      Kirschner, A. and Bertschinger, G. and Rapp, J. and Schweer,
                      B. and Noda, N.},
      title        = {{O}peration of {TEXTOR}-94 with tungsten poloidal limiters},
      journal      = {Journal of nuclear materials},
      volume       = {290-293},
      issn         = {0022-3115},
      address      = {Amsterdam [u.a.]},
      publisher    = {Elsevier Science},
      reportid     = {PreJuSER-37993},
      pages        = {947 - 952},
      year         = {2001},
      note         = {Record converted from VDB: 12.11.2012},
      abstract     = {In TEXTOR-93, experiments have been performed with the
                      upper and lower poloidal limiter blocks made of vapour
                      sprayed (VSP) tungsten (about 0.5 mm) deposited on graphite
                      with a rhenium interlayer. A series of discharge conditions
                      have been performed (density scan, scan of the auxiliary
                      heating power, radius scan). There has been found no
                      restriction for operation at any density with auxiliary
                      heating. For Ohmic conditions the same density with
                      testlimiters could be reached. Under siliconized conditions
                      no severe accumulation of tungsten in the plasma centre
                      could be detected. The blocks could in general stand surface
                      temperatures below 1700 K. Most of them survived also
                      temperatures above 3000 K without exfoliation. However, some
                      blocks showed severe damage by melting or exfoliation
                      probably due to insufficient contact of the tungsten layer
                      with the graphite. (C) 2001 Elsevier Science B.V. All rights
                      reserved.},
      keywords     = {J (WoSType)},
      cin          = {IPP-1 / IPP-2},
      ddc          = {530},
      cid          = {I:(DE-Juel1)VDB27 / I:(DE-Juel1)VDB28},
      pnm          = {Teilchen- und Energietransport in der Plasmarandschicht /
                      Wandkonditionierung und Plasma-Wand-Prozesse /
                      Instabilitäten und transportvorgänge im Plasma /
                      Verunreinigungsquellen in Tokamaks},
      pid          = {G:(DE-Juel1)FUEK48 / G:(DE-Juel1)FUEK46 /
                      G:(DE-Juel1)FUEK45 / G:(DE-Juel1)FUEK47},
      shelfmark    = {Materials Science, Multidisciplinary / Nuclear Science $\&$
                      Technology / Mining $\&$ Mineral Processing},
      typ          = {PUB:(DE-HGF)16},
      UT           = {WOS:000167676700190},
      doi          = {10.1016/S0022-3115(00)00656-5},
      url          = {https://juser.fz-juelich.de/record/37993},
}