001     808954
005     20240711085706.0
024 7 _ |a 10.1007/s11666-016-0398-4
|2 doi
024 7 _ |a 1059-9630
|2 ISSN
024 7 _ |a 1544-1016
|2 ISSN
024 7 _ |a WOS:000374328500007
|2 WOS
037 _ _ |a FZJ-2016-02464
082 _ _ |a 670
100 1 _ |a Mutter, Markus
|0 P:(DE-Juel1)157727
|b 0
|e Corresponding author
245 _ _ |a Investigations on the Initial Stress Evolution During Atmospheric Plasma Spraying of YSZ by In Situ Curvature Measurement
260 _ _ |a Boston, Mass.
|c 2016
|b Springer
336 7 _ |a article
|2 DRIVER
336 7 _ |a Output Types/Journal article
|2 DataCite
336 7 _ |a Journal Article
|b journal
|m journal
|0 PUB:(DE-HGF)16
|s 1462186656_7197
|2 PUB:(DE-HGF)
336 7 _ |a ARTICLE
|2 BibTeX
336 7 _ |a JOURNAL_ARTICLE
|2 ORCID
336 7 _ |a Journal Article
|0 0
|2 EndNote
520 _ _ |a The residual stresses within plasma-sprayed coatings are an important factor that can influence the lifetime as well as the performance in operation. The investigation of stresses evolving during deposition and post-deposition cooling for atmospheric plasma spraying of yttria-stabilized zirconia coatings using in situ measurement of the samples curvature is a powerful tool for identifying the factors that contribute to stress generation. Under various spray conditions, the first deposition pass leads to a significantly larger increase in samples curvature than the subsequent passes. It is shown in this work that the amount of curvature change at the onset of spraying is significantly influenced by the spray conditions, as well as by the substrate material. More information on the origin of this steep curvature increase at the onset of spraying was obtained by single splat experiments, which yielded information on the splat bonding behavior under various conditions. A comparison of the compressive yield strength for different substrate materials indicated the influence of substrate residual stress relaxation. Residual stress measurements using the incremental hole-drilling method and x-ray diffraction confirmed that the coating deposition affects the substrate residual stress level. The yield strength data were combined with the substrate near-surface temperature during deposition, obtained by finite element simulations, and with the measured residual stress-profile. This revealed that residual stress relaxation is the key factor for the initial curvature increase.
536 _ _ |a 113 - Methods and Concepts for Material Development (POF3-113)
|0 G:(DE-HGF)POF3-113
|c POF3-113
|f POF III
|x 0
536 _ _ |0 G:(DE-Juel1)HITEC-20170406
|x 1
|c HITEC-20170406
|a HITEC - Helmholtz Interdisciplinary Doctoral Training in Energy and Climate Research (HITEC) (HITEC-20170406)
588 _ _ |a Dataset connected to CrossRef
700 1 _ |a Mauer, Georg
|0 P:(DE-Juel1)129633
|b 1
|u fzj
700 1 _ |a Mücke, Robert
|0 P:(DE-Juel1)129641
|b 2
|u fzj
700 1 _ |a Vassen, Robert
|0 P:(DE-Juel1)129670
|b 3
700 1 _ |a Back, Hyoung Chul
|0 P:(DE-HGF)0
|b 4
700 1 _ |a Gibmeier, Jens
|0 P:(DE-HGF)0
|b 5
773 _ _ |a 10.1007/s11666-016-0398-4
|g Vol. 25, no. 4, p. 672 - 683
|0 PERI:(DE-600)2047715-6
|n 4
|p 672 - 683
|t Journal of thermal spray technology
|v 25
|y 2016
|x 1544-1016
856 4 _ |u https://juser.fz-juelich.de/record/808954/files/art_10.1007_s11666-016-0398-4.pdf
|y Restricted
856 4 _ |x icon
|u https://juser.fz-juelich.de/record/808954/files/art_10.1007_s11666-016-0398-4.gif?subformat=icon
|y Restricted
856 4 _ |x icon-1440
|u https://juser.fz-juelich.de/record/808954/files/art_10.1007_s11666-016-0398-4.jpg?subformat=icon-1440
|y Restricted
856 4 _ |x icon-180
|u https://juser.fz-juelich.de/record/808954/files/art_10.1007_s11666-016-0398-4.jpg?subformat=icon-180
|y Restricted
856 4 _ |x icon-640
|u https://juser.fz-juelich.de/record/808954/files/art_10.1007_s11666-016-0398-4.jpg?subformat=icon-640
|y Restricted
856 4 _ |x pdfa
|u https://juser.fz-juelich.de/record/808954/files/art_10.1007_s11666-016-0398-4.pdf?subformat=pdfa
|y Restricted
909 C O |o oai:juser.fz-juelich.de:808954
|p VDB
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 0
|6 P:(DE-Juel1)157727
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 1
|6 P:(DE-Juel1)129633
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 2
|6 P:(DE-Juel1)129641
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 3
|6 P:(DE-Juel1)129670
913 1 _ |a DE-HGF
|l Energieeffizienz, Materialien und Ressourcen
|1 G:(DE-HGF)POF3-110
|0 G:(DE-HGF)POF3-113
|2 G:(DE-HGF)POF3-100
|v Methods and Concepts for Material Development
|x 0
|4 G:(DE-HGF)POF
|3 G:(DE-HGF)POF3
|b Energie
914 1 _ |y 2016
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0200
|2 StatID
|b SCOPUS
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)1160
|2 StatID
|b Current Contents - Engineering, Computing and Technology
915 _ _ |a JCR
|0 StatID:(DE-HGF)0100
|2 StatID
|b J THERM SPRAY TECHN : 2013
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0150
|2 StatID
|b Web of Science Core Collection
915 _ _ |a WoS
|0 StatID:(DE-HGF)0110
|2 StatID
|b Science Citation Index
915 _ _ |a WoS
|0 StatID:(DE-HGF)0111
|2 StatID
|b Science Citation Index Expanded
915 _ _ |a IF < 5
|0 StatID:(DE-HGF)9900
|2 StatID
915 _ _ |a No Authors Fulltext
|0 StatID:(DE-HGF)0550
|2 StatID
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0199
|2 StatID
|b Thomson Reuters Master Journal List
920 _ _ |l yes
920 1 _ |0 I:(DE-Juel1)IEK-1-20101013
|k IEK-1
|l Werkstoffsynthese und Herstellungsverfahren
|x 0
980 _ _ |a journal
980 _ _ |a VDB
980 _ _ |a UNRESTRICTED
980 _ _ |a I:(DE-Juel1)IEK-1-20101013
981 _ _ |a I:(DE-Juel1)IMD-2-20101013


LibraryCollectionCLSMajorCLSMinorLanguageAuthor
Marc 21