TY - JOUR
AU - Hamaji, Y.
AU - Lee, H. T.
AU - Kreter, A.
AU - Rasinski, M.
AU - Tokitani, M.
AU - Masuzaki, S.
AU - Sagara, A.
AU - Oya, M.
AU - Ibano, K.
AU - Sakamoto, R.
AU - Ueda, Y.
AU - Möller, Sören
TI - Damage and deuterium retention of re-solidified tungsten following vertical displacement event-like heat load
JO - Nuclear materials and energy
VL - 12
SN - 2352-1791
CY - Amsterdam [u.a.]
PB - Elsevier
M1 - FZJ-2017-07927
SP - 1303 - 1307
PY - 2017
AB - Surface morphology and hydrogen isotope retention of W specimen melted with vertical displacement event-like heat load and subsequent deuterium (D) plasma exposure were studied. Applied heat loads using electron beam without raster scanning were about 190 and 230 MW/m2 in heat flux and 0.08, 0.12 and 0.16 s in duration. After the heat load application, specimens showed apparent melting spots with grain growth or dense micrometer scale convex structure. Cracks were observed only in the part with the convex structure. D retention in the melted part of specimens was not significantly larger than in the reference specimen despite large changes of surface characteristics.
LB - PUB:(DE-HGF)16
UR - <Go to ISI:>//WOS:000417293300217
DO - DOI:10.1016/j.nme.2016.11.003
UR - https://juser.fz-juelich.de/record/840394
ER -