000842559 001__ 842559
000842559 005__ 20240610121334.0
000842559 0247_ $$2doi$$a10.1002/aenm.201701663
000842559 0247_ $$2ISSN$$a1614-6832
000842559 0247_ $$2ISSN$$a1614-6840
000842559 0247_ $$2WOS$$aWOS:000424152200011
000842559 037__ $$aFZJ-2018-00778
000842559 082__ $$a600
000842559 1001_ $$0P:(DE-HGF)0$$aSchmies, Henrike$$b0
000842559 245__ $$aUnravelling Degradation Pathways of Oxide-Supported Pt Fuel Cell Nanocatalysts under In Situ Operating Conditions
000842559 260__ $$aWeinheim$$bWiley-VCH$$c2018
000842559 3367_ $$2DRIVER$$aarticle
000842559 3367_ $$2DataCite$$aOutput Types/Journal article
000842559 3367_ $$0PUB:(DE-HGF)16$$2PUB:(DE-HGF)$$aJournal Article$$bjournal$$mjournal$$s1518616373_19762
000842559 3367_ $$2BibTeX$$aARTICLE
000842559 3367_ $$2ORCID$$aJOURNAL_ARTICLE
000842559 3367_ $$00$$2EndNote$$aJournal Article
000842559 520__ $$aKnowledge of degradation pathways of catalyst/support ensembles aids the development of rational strategies to improve their stability. Here, this is exemplified using indium tin oxide (ITO)-supported Platinum nanoparticles as electrocatalysts at fuel cell (FC) cathodes under degradation protocols to mimic operating conditions in two potential regimes. The evolution of crystal structure, composition, crystallite and particle size is tracked by in situ X-ray techniques (small and wide angle scattering), metal dissolution by in situ scanning flow cell coupled with mass spectrometry (SFC ICP-MS) and Pt surface morphology by advanced electron microscopy. In a regular FC operation regime, Pt poisoning rather than Pt particle growth, agglomeration, dissolution or detachment was found to be the likely origin of the observed degradation and ORR activity losses. In the start-up regime degradation is actually suppressed and only minor losses in catalytic activity are observed. The presented data thus highlight the excellent nanoparticle stabilization and corrosion resistance of the ITO support, yet point to a degradation pathway involving Pt surface modifications by deposition of sub-monolayers of support metal ions. The identified degradation pathway of the Pt/oxide catalyst/support couple contributes to our understanding of cathode electrocatalysts for polymer electrolyte fuel cells (PEFC).
000842559 536__ $$0G:(DE-HGF)POF3-143$$a143 - Controlling Configuration-Based Phenomena (POF3-143)$$cPOF3-143$$fPOF III$$x0
000842559 588__ $$aDataset connected to CrossRef
000842559 7001_ $$0P:(DE-HGF)0$$aBergmann, Arno$$b1
000842559 7001_ $$0P:(DE-HGF)0$$aDrnec, Jakub$$b2
000842559 7001_ $$0P:(DE-HGF)0$$aWang, Guanxiong$$b3
000842559 7001_ $$0P:(DE-HGF)0$$aTeschner, Detre$$b4
000842559 7001_ $$0P:(DE-HGF)0$$aKühl, Stefanie$$b5
000842559 7001_ $$0P:(DE-HGF)0$$aSandbeck, Daniel J. S.$$b6
000842559 7001_ $$0P:(DE-Juel1)168567$$aCherevko, Serhiy$$b7
000842559 7001_ $$0P:(DE-Juel1)161464$$aGocyla, Martin$$b8
000842559 7001_ $$0P:(DE-Juel1)165174$$aShviro, Meital$$b9
000842559 7001_ $$0P:(DE-Juel1)130695$$aHeggen, Marc$$b10
000842559 7001_ $$0P:(DE-HGF)0$$aRamani, Vijay$$b11
000842559 7001_ $$0P:(DE-Juel1)144121$$aDunin-Borkowski, Rafal$$b12
000842559 7001_ $$0P:(DE-HGF)0$$aMayrhofer, Karl J. J.$$b13
000842559 7001_ $$0P:(DE-HGF)0$$aStrasser, Peter$$b14$$eCorresponding author
000842559 773__ $$0PERI:(DE-600)2594556-7$$a10.1002/aenm.201701663$$gp. 1701663 -$$n4$$p1701663 $$tAdvanced energy materials$$v8$$x1614-6832$$y2018
000842559 909CO $$ooai:juser.fz-juelich.de:842559$$pVDB
000842559 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)168567$$aForschungszentrum Jülich$$b7$$kFZJ
000842559 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)165174$$aForschungszentrum Jülich$$b9$$kFZJ
000842559 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)130695$$aForschungszentrum Jülich$$b10$$kFZJ
000842559 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)144121$$aForschungszentrum Jülich$$b12$$kFZJ
000842559 9131_ $$0G:(DE-HGF)POF3-143$$1G:(DE-HGF)POF3-140$$2G:(DE-HGF)POF3-100$$3G:(DE-HGF)POF3$$4G:(DE-HGF)POF$$aDE-HGF$$bEnergie$$lFuture Information Technology - Fundamentals, Novel Concepts and Energy Efficiency (FIT)$$vControlling Configuration-Based Phenomena$$x0
000842559 9141_ $$y2018
000842559 915__ $$0StatID:(DE-HGF)0200$$2StatID$$aDBCoverage$$bSCOPUS
000842559 915__ $$0StatID:(DE-HGF)0300$$2StatID$$aDBCoverage$$bMedline
000842559 915__ $$0StatID:(DE-HGF)0100$$2StatID$$aJCR$$bADV ENERGY MATER : 2015
000842559 915__ $$0StatID:(DE-HGF)0199$$2StatID$$aDBCoverage$$bThomson Reuters Master Journal List
000842559 915__ $$0StatID:(DE-HGF)0111$$2StatID$$aWoS$$bScience Citation Index Expanded
000842559 915__ $$0StatID:(DE-HGF)0150$$2StatID$$aDBCoverage$$bWeb of Science Core Collection
000842559 915__ $$0StatID:(DE-HGF)1150$$2StatID$$aDBCoverage$$bCurrent Contents - Physical, Chemical and Earth Sciences
000842559 915__ $$0StatID:(DE-HGF)1160$$2StatID$$aDBCoverage$$bCurrent Contents - Engineering, Computing and Technology
000842559 915__ $$0StatID:(DE-HGF)9915$$2StatID$$aIF >= 15$$bADV ENERGY MATER : 2015
000842559 920__ $$lyes
000842559 9201_ $$0I:(DE-Juel1)ER-C-1-20170209$$kER-C-1$$lPhysik Nanoskaliger Systeme$$x0
000842559 9201_ $$0I:(DE-Juel1)PGI-5-20110106$$kPGI-5$$lMikrostrukturforschung$$x1
000842559 980__ $$ajournal
000842559 980__ $$aVDB
000842559 980__ $$aI:(DE-Juel1)ER-C-1-20170209
000842559 980__ $$aI:(DE-Juel1)PGI-5-20110106
000842559 980__ $$aUNRESTRICTED
000842559 981__ $$aI:(DE-Juel1)ER-C-1-20170209