title = {{O}bservation of chemically protected polydimethylsiloxane:
towards crack-free {PDMS}},
journal = {Soft matter},
volume = {13},
number = {37},
issn = {1744-683X},
address = {London},
publisher = {Royal Soc. of Chemistry},
reportid = {FZJ-2018-03413},
pages = {6297- 6303},
year = {2017},
abstract = {The current modification of polydimethylsiloxane (PDMS)
substrates via oxygen plasma treatment causes surface
cracks. Here, we demonstrate a method to prevent crack
formation by chemical treatment. Chemical modification
renders the surface hydrophilic for several days and is
effective in preserving the elasticity of the PDMS surface
at the nanoscale level.},
cin = {ICS-8 / JARA-SOFT},
ddc = {530},
cid = {I:(DE-Juel1)ICS-8-20110106 / $I:(DE-82)080008_20150909$},
pnm = {552 - Engineering Cell Function (POF3-552)},
pid = {G:(DE-HGF)POF3-552},
typ = {PUB:(DE-HGF)16},
pubmed = {pmid:28920620},
UT = {WOS:000411863200003},
doi = {10.1039/C7SM01457K},
url = {https://juser.fz-juelich.de/record/848141},
}