000850110 1001_ $$0P:(DE-Juel1)161483$$aThaler, Florian$$b0$$eCorresponding author
000850110 1112_ $$a13th European SOFC & SOE Forum 2018$$cLucerne$$d2018-07-03 - 2018-07-06$$gEFCF'18$$wSwitzerland
000850110 245__ $$aRedox Cycling of Ni/YSZ and Ni/GDC Anodes for Metal-Supported Fuel Cells
000850110 260__ $$aLucerne, Switzerland$$bEuropean Fuel Cell Forum AG$$c2018
000850110 300__ $$a18-27
000850110 3367_ $$2ORCID$$aCONFERENCE_PAPER
000850110 3367_ $$033$$2EndNote$$aConference Paper
000850110 3367_ $$2BibTeX$$aINPROCEEDINGS
000850110 3367_ $$2DRIVER$$aconferenceObject
000850110 3367_ $$2DataCite$$aOutput Types/Conference Paper
000850110 3367_ $$0PUB:(DE-HGF)8$$2PUB:(DE-HGF)$$aContribution to a conference proceedings$$bcontrib$$mcontrib$$s1536675169_9692
000850110 3367_ $$0PUB:(DE-HGF)7$$2PUB:(DE-HGF)$$aContribution to a book$$mcontb
000850110 4900_ $$v13
000850110 520__ $$aMetal-supported fuel cells (MSCs) are promising candidates for non-stationary applications like auxiliary power units or range extenders in battery electric vehicles. They are attractive due to their potential to withstand fast thermal cycles and vibrations during cell operation. In addition, they have to withstand redox cycles, which might occur during start-up and shut-down of the fuel cell stack. Recently, a novel nickel/gadolinium doped ceria anode (Ni/GDC) was introduced in the metal-supported fuel cell concept of Plansee SE which almost tripled current density compared to the standard cell concept with a Ni/YSZ anode. In the present work, both cell concepts were compared regarding their ability to withstand harsh redox cycles. Therefore, after initial check at 750 °C, cell performance of button cells after controlled redox cycles was investigated at different temperature steps respectively. Re-oxidation temperature of the anodes was varied between 300 and 700 °C for 10 min in air. Afterwards, reduction of the anode was conducted by purging anode side with N2 for 10 min and then going back to standard cell operation conditions with H2 supply. The response of cell performance on redox cycling was recorded continuously. While standard MSCs with Ni/YSZ anode showed a strong degradation after a few cycles if the oxidation was conducted at temperatures above 600 °C, novel MSCs with Ni/GDC anode showed a remarkable resistance against re-oxidation. For a deeper understanding of this behavior, microstructural investigation of the Ni/GDC anode and the adjacent electrolyte was performed within the tested cells by FE-SEM and FIB-SEM 3D structure analysis. Furthermore, electrochemical behavior of Ni/GDC anode was investigated at a larger cycle number of up to 50 redox cycles with 2 h air supply each.
000850110 536__ $$0G:(DE-HGF)POF3-135$$a135 - Fuel Cells (POF3-135)$$cPOF3-135$$fPOF III$$x0
000850110 536__ $$0G:(DE-Juel1)SOFC-20140602$$aSOFC - Solid Oxide Fuel Cell (SOFC-20140602)$$cSOFC-20140602$$fSOFC$$x1
000850110 7001_ $$0P:(DE-Juel1)161337$$aUdomsilp, David$$b1
000850110 7001_ $$0P:(DE-HGF)0$$aSchafbauer, Wolfgang$$b2
000850110 7001_ $$0P:(DE-HGF)0$$aBischof, Cornelia$$b3
000850110 7001_ $$0P:(DE-HGF)0$$aFukuyama$$b4
000850110 7001_ $$0P:(DE-HGF)0$$aMiura, Yohei$$b5
000850110 7001_ $$0P:(DE-HGF)0$$aKawabuchi, Mari$$b6
000850110 7001_ $$0P:(DE-HGF)0$$aTaniguchi, Schunsuke$$b7
000850110 7001_ $$0P:(DE-HGF)0$$aTakemiya, Satoshi$$b8
000850110 7001_ $$0P:(DE-HGF)0$$aOpitz, Alexander Karl$$b9
000850110 7001_ $$0P:(DE-Juel1)129591$$aBram, Martin$$b10$$ufzj
000850110 773__ $$nB1202$$p18-27$$vChapter 12
000850110 909CO $$ooai:juser.fz-juelich.de:850110$$pVDB
000850110 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)161483$$aForschungszentrum Jülich$$b0$$kFZJ
000850110 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)161337$$aForschungszentrum Jülich$$b1$$kFZJ
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b2$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Plansee SE, Austria$$b2
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b3$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Plansee SE, Austria$$b3
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b4$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Nissan Motor Co, Japan$$b4
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b5$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Nissan Motor Co, Japan$$b5
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b6$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Nissan Motor Co, Japan$$b6
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b7$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Kyushu University, Japan$$b7
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b8$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Kyushu University, Japan$$b8
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$aExternal Institute$$b9$$kExtern
000850110 9101_ $$0I:(DE-HGF)0$$6P:(DE-HGF)0$$a Vienna University of Technology, Austria$$b9
000850110 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)129591$$aForschungszentrum Jülich$$b10$$kFZJ
000850110 9131_ $$0G:(DE-HGF)POF3-135$$1G:(DE-HGF)POF3-130$$2G:(DE-HGF)POF3-100$$3G:(DE-HGF)POF3$$4G:(DE-HGF)POF$$aDE-HGF$$bEnergie$$lSpeicher und vernetzte Infrastrukturen$$vFuel Cells$$x0
000850110 9141_ $$y2018
000850110 920__ $$lyes
000850110 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$kIEK-1$$lWerkstoffsynthese und Herstellungsverfahren$$x0
000850110 980__ $$acontrib
000850110 980__ $$aVDB
000850110 980__ $$acontb
000850110 980__ $$aI:(DE-Juel1)IEK-1-20101013
000850110 980__ $$aUNRESTRICTED
000850110 981__ $$aI:(DE-Juel1)IMD-2-20101013