@INPROCEEDINGS{Ma:851085,
      author       = {Ma, Qianli and Tsai, Chih-Long and Tietz, Frank},
      title        = {{A} room-temperature full-ceramic sodium-ion battery based
                      on {N}a3+x{Z}r2{S}i2+x{P}1-x{O}12 as sodium superionic
                      conductor},
      reportid     = {FZJ-2018-04793},
      year         = {2018},
      abstract     = {Despite of huge efforts, the lack of suitable candidate for
                      electrolytes still impedes the development of
                      all-solid-state Na batteries. Na3+xZr2Si2+xP1-xO12 (-0.2 ≤
                      x ≤ 0.2) are the very first composition series of NASICONs
                      discovered 40 years ago and were reported having a total
                      Na-ion conductivity of ~10-4 S cm-1 at room temperature. In
                      the present study, this composition series is reconsidered
                      and the focusing range of stoichiometry has been varied from
                      x = 0 to x = 0.6. A solution-assisted solid-state reaction
                      method is applied for powder preparation. Surprisingly, a
                      total conductivity of over 5 × 10-3 S cm-1 is achieved for
                      Na3.4Zr2Si2.4P0.6O12 at 25 °C, which is the best value of
                      all reported polycrystalline Na-ion conductors. A bulk
                      conductivity of about 1.5 × 10-2 S cm-1 is also revealed by
                      high frequency impedance spectroscopy up to 3 GHz for
                      Na3.4Zr2Si2.4P0.6O12 at 25 °C. The parameters influencing
                      the total conductivity are discussed in detail. Benefitted
                      from the superior total conductivity of
                      Na3.4Zr2Si2.4P0.6O12, a full-ceramic cell has been
                      fabricated and tested at 28 °C with good cycling
                      performance. To our knowledge, this is the first full
                      ceramic Na-ion battery which has been operated at room
                      temperature.},
      month         = {Jul},
      date          = {2018-07-22},
      organization  = {12th International Conference on
                       Ceramic Materials and Components for
                       Energy and Environmental Applications,
                       Singapore (Singapore), 22 Jul 2018 - 27
                       Jul 2018},
      subtyp        = {Invited},
      cin          = {IEK-1},
      cid          = {I:(DE-Juel1)IEK-1-20101013},
      pnm          = {131 - Electrochemical Storage (POF3-131) / SOFC - Solid
                      Oxide Fuel Cell (SOFC-20140602)},
      pid          = {G:(DE-HGF)POF3-131 / G:(DE-Juel1)SOFC-20140602},
      typ          = {PUB:(DE-HGF)6},
      url          = {https://juser.fz-juelich.de/record/851085},
}