100 1 _ |a Holtstiege, Florian
|0 P:(DE-HGF)0
|b 0
245 _ _ |a Running out of lithium? A route to differentiate between capacity losses and active lithium losses in lithium-ion batteries
260 _ _ |a Cambridge
|c 2017
|b RSC Publ.
336 7 _ |a article
|2 DRIVER
336 7 _ |a Output Types/Journal article
|2 DataCite
336 7 _ |a Journal Article
|b journal
|m journal
|0 PUB:(DE-HGF)16
|s 1534312847_7415
|2 PUB:(DE-HGF)
336 7 _ |a ARTICLE
|2 BibTeX
336 7 _ |a JOURNAL_ARTICLE
|2 ORCID
336 7 _ |a Journal Article
|0 0
|2 EndNote
520 _ _ |a Active lithium loss (ALL) resulting in a capacity loss (QALL), which is caused by lithium consuming parasitic reactions like SEI formation, is a major reason for capacity fading and, thus, for a reduction of the usable energy density of lithium-ion batteries (LIBs). QALL is often equated with the accumulated irreversible capacity (QAIC). However, QAIC is also influenced by non-lithium consuming parasitic reactions, which do not reduce the active lithium content of the cell, but induce a parasitic current. In this work, a novel approach is proposed in order to differentiate between QAIC and QALL. The determination of QALL is based on the remaining active lithium content of a given cell, which can be determined by de-lithiation of the cathode with the help of the reference electrode of a three-electrode set-up. Lithium non-consuming parasitic reactions, which do not influence the active lithium content have no influence on this determination. In order to evaluate this novel approach, three different anode materials (graphite, carbon spheres and a silicon/graphite composite) were investigated. It is shown that during the first charge/discharge cycles QALL is described moderately well by QAIC. However, the difference between QAIC and QALL rises with increasing cycle number. With this approach, a differentiation between “simple” irreversible capacities and truly detrimental “active Li losses” is possible and, thus, Coulombic efficiency can be directly related to the remaining useable cell capacity for the first time. Overall, the exact determination of the remaining active lithium content of the cell is of great importance, because it allows a statement on whether the reduction in lithium content is crucial for capacity fading or whether the fading is related to other degradation mechanisms such as material or electrode failure.
536 _ _ |a 131 - Electrochemical Storage (POF3-131)
|0 G:(DE-HGF)POF3-131
|c POF3-131
|f POF III
|x 0
588 _ _ |a Dataset connected to CrossRef
700 1 _ |a Wilken, Andrea
|0 P:(DE-HGF)0
|b 1
700 1 _ |a Winter, Martin
|0 P:(DE-Juel1)166130
|b 2
|e Corresponding author
|u fzj
700 1 _ |a Placke, Tobias
|0 0000-0002-2097-5193
|b 3
|e Corresponding author
773 _ _ |a 10.1039/C7CP05405J
|g Vol. 19, no. 38, p. 25905 - 25918
|0 PERI:(DE-600)1476244-4
|n 38
|p 25905 - 25918
|t Physical chemistry, chemical physics
|v 19
|y 2017
|x 1463-9076
856 4 _ |u https://juser.fz-juelich.de/record/851135/files/c7cp05405j.pdf
|y Restricted
856 4 _ |u https://juser.fz-juelich.de/record/851135/files/c7cp05405j.gif?subformat=icon
|x icon
|y Restricted
856 4 _ |u https://juser.fz-juelich.de/record/851135/files/c7cp05405j.jpg?subformat=icon-1440
|x icon-1440
|y Restricted
856 4 _ |u https://juser.fz-juelich.de/record/851135/files/c7cp05405j.jpg?subformat=icon-180
|x icon-180
|y Restricted
856 4 _ |u https://juser.fz-juelich.de/record/851135/files/c7cp05405j.jpg?subformat=icon-640
|x icon-640
|y Restricted
856 4 _ |u https://juser.fz-juelich.de/record/851135/files/c7cp05405j.pdf?subformat=pdfa
|x pdfa
|y Restricted
909 C O |o oai:juser.fz-juelich.de:851135
|p VDB
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 2
|6 P:(DE-Juel1)166130
913 1 _ |a DE-HGF
|l Speicher und vernetzte Infrastrukturen
|1 G:(DE-HGF)POF3-130
|0 G:(DE-HGF)POF3-131
|2 G:(DE-HGF)POF3-100
|v Electrochemical Storage
|x 0
|4 G:(DE-HGF)POF
|3 G:(DE-HGF)POF3
|b Energie
914 1 _ |y 2018
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0200
|2 StatID
|b SCOPUS
915 _ _ |a Nationallizenz
|0 StatID:(DE-HGF)0420
|2 StatID
915 _ _ |a JCR
|0 StatID:(DE-HGF)0100
|2 StatID
|b PHYS CHEM CHEM PHYS : 2015
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0200
|2 StatID
|b SCOPUS
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0300
|2 StatID
|b Medline
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0310
|2 StatID
|b NCBI Molecular Biology Database
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0199
|2 StatID
|b Thomson Reuters Master Journal List
915 _ _ |a WoS
|0 StatID:(DE-HGF)0110
|2 StatID
|b Science Citation Index
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0150
|2 StatID
|b Web of Science Core Collection
915 _ _ |a WoS
|0 StatID:(DE-HGF)0111
|2 StatID
|b Science Citation Index Expanded
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)1150
|2 StatID
|b Current Contents - Physical, Chemical and Earth Sciences
915 _ _ |a IF < 5
|0 StatID:(DE-HGF)9900
|2 StatID
920 1 _ |0 I:(DE-Juel1)IEK-12-20141217
|k IEK-12
|l Helmholtz-Institut Münster Ionenleiter für Energiespeicher
|x 0
980 _ _ |a journal
980 _ _ |a VDB
980 _ _ |a I:(DE-Juel1)IEK-12-20141217
980 _ _ |a UNRESTRICTED
981 _ _ |a I:(DE-Juel1)IMD-4-20141217


LibraryCollectionCLSMajorCLSMinorLanguageAuthor
Marc 21