author = {Gonzalez-Julian, Jesus and Go, Teresa and Mack, Daniel E.
and Vaßen, Robert},
title = {{E}nvironmental resistance of {C}r 2 {A}l{C} {MAX} phase
under thermal gradient loading using a burner rig},
journal = {Journal of the American Ceramic Society},
volume = {101},
number = {5},
issn = {0002-7820},
address = {Oxford [u.a.]},
publisher = {Wiley-Blackwell},
reportid = {FZJ-2018-04907},
pages = {1841 - 1846},
year = {2018},
abstract = {Dense Cr2AlC materials were tested under a gradient loading
for the first time using a burner rig. The severe thermal
cycling conditions consist of 500 short cycles at 1200°C,
with an accumulative time at the maximal temperature of more
than 29 hours. The samples showed no visible damage under
these conditions due to the formation of an outer protective
α‐Al2O3 layer, which shows a strong adhesion with the
Cr2AlC substrate. No cracks, delamination or damage were
observed at the interface between the different layers. This
excellent response under cyclic loading shows the excellent
potential of Cr2AlC compounds for high‐temperature
applications.},
cin = {IEK-1},
ddc = {660},
cid = {I:(DE-Juel1)IEK-1-20101013},
pnm = {113 - Methods and Concepts for Material Development
(POF3-113)},
pid = {G:(DE-HGF)POF3-113},
typ = {PUB:(DE-HGF)16},
UT = {WOS:000426513900009},
doi = {10.1111/jace.15425},
url = {https://juser.fz-juelich.de/record/851207},
}