000858372 1001_ $$00000-0003-2914-0237$$aHuang, Taihong$$b0
000858372 245__ $$aEffect of Titanium Addition on Alumina Growth Mechanism on Yttria-Containing FeCrAl-Base Alloy
000858372 260__ $$aDordrecht [u.a.]$$bSpringer Science + Business Media B.V$$c2018
000858372 3367_ $$2DRIVER$$aarticle
000858372 3367_ $$2DataCite$$aOutput Types/Journal article
000858372 3367_ $$0PUB:(DE-HGF)16$$2PUB:(DE-HGF)$$aJournal Article$$bjournal$$mjournal$$s1544522314_28838
000858372 3367_ $$2BibTeX$$aARTICLE
000858372 3367_ $$2ORCID$$aJOURNAL_ARTICLE
000858372 3367_ $$00$$2EndNote$$aJournal Article
000858372 520__ $$aFeCrAl-base alloys are well known for their excellent oxidation resistance due to formation of a slowly growing alumina surface scale during high-temperature service. The actual scale growth mechanism and especially adherence are strongly affected by the presence of oxygen-active elements such as yttrium, titanium or hafnium. In the present study, the effect of titanium addition on the scale growth mechanisms of an yttrium oxide dispersion-strengthened FeCrAl base alloy was studied during oxidation at 1200 °C in Ar–O2. For microstructural characterization results of scanning electron microscopy and electron backscatter diffraction were combined with X-ray diffraction data. Scale growth mechanisms were investigated by two-stage oxidation using 18O tracer with subsequent scale analyses using secondary neutrals mass spectrometry. The scale on the alloy without intentionally added titanium grew virtually exclusively by oxygen diffusion along oxide grain boundaries and exhibited a columnar structure with the grain size increasing in growth direction. The addition of titanium resulted in formation of an outer oxide zone of equiaxed grains on top of the inner columnar part. The equiaxed grains increased in size with increasing exposure time. Comparison with the tracer studies revealed that the titanium-induced equiaxed zone was the result of outer scale growth. Mechanisms for the initiation of outward aluminium transport are discussed. Indications were found that the effect of titanium on the scale growth mechanisms already occurred for titanium additions as low as 0.02 wt%.
000858372 536__ $$0G:(DE-HGF)POF3-111$$a111 - Efficient and Flexible Power Plants (POF3-111)$$cPOF3-111$$fPOF III$$x0
000858372 588__ $$aDataset connected to CrossRef
000858372 7001_ $$0P:(DE-Juel1)129766$$aNaumenko, Dmitry$$b1$$eCorresponding author
000858372 7001_ $$0P:(DE-HGF)0$$aSong, Peng$$b2
000858372 7001_ $$0P:(DE-HGF)0$$aLu, Jiansheng$$b3
000858372 7001_ $$0P:(DE-HGF)0$$aQuadakkers, Willem Joseph$$b4
000858372 773__ $$0PERI:(DE-600)2018581-9$$a10.1007/s11085-018-9861-6$$gVol. 90, no. 5-6, p. 671 - 690$$n5-6$$p671 - 690$$tOxidation of metals$$v90$$x1573-4889$$y2018
000858372 8564_ $$uhttps://juser.fz-juelich.de/record/858372/files/Huang2018_Article_EffectOfTitaniumAdditionOnAlum.pdf$$yRestricted
000858372 8564_ $$uhttps://juser.fz-juelich.de/record/858372/files/Huang2018_Article_EffectOfTitaniumAdditionOnAlum.pdf?subformat=pdfa$$xpdfa$$yRestricted
000858372 909CO $$ooai:juser.fz-juelich.de:858372$$pVDB
000858372 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)129766$$aForschungszentrum Jülich$$b1$$kFZJ
000858372 9131_ $$0G:(DE-HGF)POF3-111$$1G:(DE-HGF)POF3-110$$2G:(DE-HGF)POF3-100$$3G:(DE-HGF)POF3$$4G:(DE-HGF)POF$$aDE-HGF$$bEnergie$$lEnergieeffizienz, Materialien und Ressourcen$$vEfficient and Flexible Power Plants$$x0
000858372 9141_ $$y2018
000858372 915__ $$0StatID:(DE-HGF)0420$$2StatID$$aNationallizenz
000858372 915__ $$0StatID:(DE-HGF)0200$$2StatID$$aDBCoverage$$bSCOPUS
000858372 915__ $$0StatID:(DE-HGF)0100$$2StatID$$aJCR$$bOXID MET : 2017
000858372 915__ $$0StatID:(DE-HGF)0600$$2StatID$$aDBCoverage$$bEbsco Academic Search
000858372 915__ $$0StatID:(DE-HGF)0030$$2StatID$$aPeer Review$$bASC
000858372 915__ $$0StatID:(DE-HGF)0199$$2StatID$$aDBCoverage$$bClarivate Analytics Master Journal List
000858372 915__ $$0StatID:(DE-HGF)0110$$2StatID$$aWoS$$bScience Citation Index
000858372 915__ $$0StatID:(DE-HGF)0150$$2StatID$$aDBCoverage$$bWeb of Science Core Collection
000858372 915__ $$0StatID:(DE-HGF)0111$$2StatID$$aWoS$$bScience Citation Index Expanded
000858372 915__ $$0StatID:(DE-HGF)1160$$2StatID$$aDBCoverage$$bCurrent Contents - Engineering, Computing and Technology
000858372 915__ $$0StatID:(DE-HGF)9900$$2StatID$$aIF < 5
000858372 9201_ $$0I:(DE-Juel1)IEK-2-20101013$$kIEK-2$$lWerkstoffstruktur und -eigenschaften$$x0
000858372 980__ $$ajournal
000858372 980__ $$aVDB
000858372 980__ $$aI:(DE-Juel1)IEK-2-20101013
000858372 980__ $$aUNRESTRICTED
000858372 981__ $$aI:(DE-Juel1)IMD-1-20101013