Home > Publications database > Performance of wear resistant MCrAlY coatings with oxide dispersion strengthening > print |
001 | 866332 | ||
005 | 20240708132829.0 | ||
024 | 7 | _ | |a 10.1016/j.wear.2019.203116 |2 doi |
024 | 7 | _ | |a 0043-1648 |2 ISSN |
024 | 7 | _ | |a 1873-2577 |2 ISSN |
024 | 7 | _ | |a 2128/24022 |2 Handle |
024 | 7 | _ | |a WOS:000513001800001 |2 WOS |
037 | _ | _ | |a FZJ-2019-05488 |
041 | _ | _ | |a English |
082 | _ | _ | |a 670 |
100 | 1 | _ | |a Bolelli, Giovanni |0 P:(DE-HGF)0 |b 0 |e Corresponding author |
245 | _ | _ | |a Performance of wear resistant MCrAlY coatings with oxide dispersion strengthening |
260 | _ | _ | |a Amsterdam [u.a.] |c 2020 |b Elsevier Science |
336 | 7 | _ | |a article |2 DRIVER |
336 | 7 | _ | |a Output Types/Journal article |2 DataCite |
336 | 7 | _ | |a Journal Article |b journal |m journal |0 PUB:(DE-HGF)16 |s 1579867055_19357 |2 PUB:(DE-HGF) |
336 | 7 | _ | |a ARTICLE |2 BibTeX |
336 | 7 | _ | |a JOURNAL_ARTICLE |2 ORCID |
336 | 7 | _ | |a Journal Article |0 0 |2 EndNote |
520 | _ | _ | |a Aiming to devise suitable materials for sliding wear protection at high temperature, aluminium oxide-dispersion strengthened (ODS) CoNiCrAlY coatings were manufactured by vacuum plasma spraying (VPS). Feedstock materials were ball-milled powders with 2, 10 and 30 wt% Al2O3 content. The ball-on-disc sliding wear behaviour of the coatings was tested at 750 °C against an Al2O3 counterpart, and compared to a pure CoNiCrAlY coating (obtained from a commercial feedstock not subjected to ball milling) and to an uncoated Ni-base superalloy.Sliding wear rates decrease from the uncoated superalloy (≈3 × 10−5 mm3/(N·m)) to the pure CoNiCrAlY coating (≈2 × 10−5 mm3/(N·m)) and to the ODS ones, with the notable exception of the 10 wt% Al2O3-containing sample.Analyses of worn samples indicate that pure CoNiCrAlY is subject to severe adhesive wear, mitigated by the formation of a thick (>1 μm) “glaze” layer via compaction and (probable) sintering of tribo-oxidized debris particles. Addition of Al2O3 particles to the CoNiCrAlY matrix can either enhance or worsen the “glaze” stability. Specifically, a coating strengthened with 30 wt% Al2O3 provides an especially good mechanical support to the “glaze”. This produces beneficial effects resulting in a particularly low wear rate of ≈3 × 10−6 mm3/(N·m). |
536 | _ | _ | |a 113 - Methods and Concepts for Material Development (POF3-113) |0 G:(DE-HGF)POF3-113 |c POF3-113 |f POF III |x 0 |
588 | _ | _ | |a Dataset connected to CrossRef |
700 | 1 | _ | |a Vorkötter, Christoph |0 P:(DE-Juel1)171660 |b 1 |u fzj |
700 | 1 | _ | |a Lusvarghi, Luca |0 P:(DE-HGF)0 |b 2 |
700 | 1 | _ | |a Morelli, Stefania |0 P:(DE-Juel1)180272 |b 3 |u fzj |
700 | 1 | _ | |a Testa, Veronica |0 P:(DE-HGF)0 |b 4 |
700 | 1 | _ | |a Vaßen, Robert |0 P:(DE-Juel1)129670 |b 5 |u fzj |
773 | _ | _ | |a 10.1016/j.wear.2019.203116 |g p. 203116 - |0 PERI:(DE-600)1501123-9 |p 203116 |t Wear |v 444-445 |y 2020 |x 0043-1648 |
856 | 4 | _ | |y Published on 2019-11-08. Available in OpenAccess from 2021-11-08. |u https://juser.fz-juelich.de/record/866332/files/Post%20Referee%20Version.pdf |
856 | 4 | _ | |y Published on 2019-11-08. Available in OpenAccess from 2021-11-08. |x pdfa |u https://juser.fz-juelich.de/record/866332/files/Post%20Referee%20Version.pdf?subformat=pdfa |
909 | C | O | |o oai:juser.fz-juelich.de:866332 |p openaire |p open_access |p VDB |p driver |p dnbdelivery |
910 | 1 | _ | |a Forschungszentrum Jülich |0 I:(DE-588b)5008462-8 |k FZJ |b 1 |6 P:(DE-Juel1)171660 |
910 | 1 | _ | |a Forschungszentrum Jülich |0 I:(DE-588b)5008462-8 |k FZJ |b 3 |6 P:(DE-Juel1)180272 |
910 | 1 | _ | |a Forschungszentrum Jülich |0 I:(DE-588b)5008462-8 |k FZJ |b 5 |6 P:(DE-Juel1)129670 |
913 | 1 | _ | |a DE-HGF |l Energieeffizienz, Materialien und Ressourcen |1 G:(DE-HGF)POF3-110 |0 G:(DE-HGF)POF3-113 |2 G:(DE-HGF)POF3-100 |v Methods and Concepts for Material Development |x 0 |4 G:(DE-HGF)POF |3 G:(DE-HGF)POF3 |b Energie |
914 | 1 | _ | |y 2020 |
915 | _ | _ | |a DBCoverage |0 StatID:(DE-HGF)0200 |2 StatID |b SCOPUS |
915 | _ | _ | |a DBCoverage |0 StatID:(DE-HGF)1160 |2 StatID |b Current Contents - Engineering, Computing and Technology |
915 | _ | _ | |a DBCoverage |0 StatID:(DE-HGF)0600 |2 StatID |b Ebsco Academic Search |
915 | _ | _ | |a Embargoed OpenAccess |0 StatID:(DE-HGF)0530 |2 StatID |
915 | _ | _ | |a JCR |0 StatID:(DE-HGF)0100 |2 StatID |b WEAR : 2017 |
915 | _ | _ | |a DBCoverage |0 StatID:(DE-HGF)0150 |2 StatID |b Web of Science Core Collection |
915 | _ | _ | |a WoS |0 StatID:(DE-HGF)0110 |2 StatID |b Science Citation Index |
915 | _ | _ | |a WoS |0 StatID:(DE-HGF)0111 |2 StatID |b Science Citation Index Expanded |
915 | _ | _ | |a IF < 5 |0 StatID:(DE-HGF)9900 |2 StatID |
915 | _ | _ | |a Peer Review |0 StatID:(DE-HGF)0030 |2 StatID |b ASC |
915 | _ | _ | |a DBCoverage |0 StatID:(DE-HGF)0300 |2 StatID |b Medline |
915 | _ | _ | |a DBCoverage |0 StatID:(DE-HGF)0199 |2 StatID |b Clarivate Analytics Master Journal List |
920 | 1 | _ | |0 I:(DE-Juel1)IEK-1-20101013 |k IEK-1 |l Werkstoffsynthese und Herstellungsverfahren |x 0 |
980 | 1 | _ | |a FullTexts |
980 | _ | _ | |a journal |
980 | _ | _ | |a VDB |
980 | _ | _ | |a UNRESTRICTED |
980 | _ | _ | |a I:(DE-Juel1)IEK-1-20101013 |
981 | _ | _ | |a I:(DE-Juel1)IMD-2-20101013 |
Library | Collection | CLSMajor | CLSMinor | Language | Author |
---|