@ARTICLE{Ferraris:877537,
      author       = {Ferraris, M. and De la Pierre, S. and Sabato, A. G. and
                      Smeacetto, F. and Javed, H. and Walter, C. and Malzbender,
                      J.},
      title        = {{T}orsional shear strength behavior of advanced
                      glass-ceramic sealants for {SOFC}/{SOEC} applications},
      journal      = {Journal of the European Ceramic Society},
      volume       = {40},
      number       = {12},
      issn         = {0955-2219},
      address      = {Amsterdam [u.a.]},
      publisher    = {Elsevier Science},
      reportid     = {FZJ-2020-02273},
      pages        = {4067-4075},
      year         = {2020},
      abstract     = {Since reliable long term operation of SOFC and SOEC devices
                      depends critically on the mechanical behavior of the sealant
                      material, the current work focuses on the characterization
                      of the shear strength by a torsion test of two different
                      glass-ceramic sealants that are used to join Crofer22APU
                      substrates in an application relevant configuration. The two
                      glass-ceramic sealants differ in terms of characteristic
                      temperatures and crystalline phases with possible
                      impications on the joining behavior. Statistically identical
                      shear stress values were measured at room temperature for
                      joined hourglasses of different size with both sealants,
                      thus confirming a size independence of the measured strength
                      values. Experimental post-test examination results confirm
                      that the interfaces play a strong role regarding the
                      measured shear strength and provide important insights with
                      respect to integration of metallic and glass-ceramic
                      components in SOFC/SOEC stacks.},
      cin          = {IEK-2},
      ddc          = {660},
      cid          = {I:(DE-Juel1)IEK-2-20101013},
      pnm          = {135 - Fuel Cells (POF3-135)},
      pid          = {G:(DE-HGF)POF3-135},
      typ          = {PUB:(DE-HGF)16},
      UT           = {WOS:000541149500030},
      doi          = {10.1016/j.jeurceramsoc.2020.04.034},
      url          = {https://juser.fz-juelich.de/record/877537},
}