      title        = {{D}etermination of sintering stress and bulk viscosity from
                      sinter-forging and {X}-ray microtomography methods: a
                      {R}eview},
      journal      = {Materials today / Proceedings},
      volume       = {16},
      issn         = {2214-7853},
      address      = {Amsterdam [u.a.]},
      publisher    = {Elsevier},
      reportid     = {FZJ-2021-03940},
      pages        = {42 - 48},
      year         = {2019},
      abstract     = {Sintering stress and bulk viscosity for viscous sintering
                      of glass were determined by two methods; sinter-forging and
                      X-ray microtomography methods. Calcium aluminosilicate (CAS)
                      glass with the diameter of 2.7 µm was chosen in
                      sinter-forging experiment, while soda-lime glass with the
                      diameter of 160 μm was observed by X-ray microtomography.
                      Sintering stress of CAS glass and soda-lime glass was
                      normalized by surface energy and the initial particle size.
                      The normalized sintering stress of CAS glass determined by
                      sinter-forging method was in fair agreement with values
                      estimated from the X-ray microtomography data of soda-lime
                      glass, despite the differences in particle shape and
                      chemical composition. Bulk viscosity were also normalized by
                      glass viscosity, and the normalized bulk viscosity obtained
                      by sinter-forging method agreed fairly well with that
                      estimated by X-ray microtomography method.},
      cin          = {IEK-1 / JARA-ENERGY},
      ddc          = {670},
      cid          = {I:(DE-Juel1)IEK-1-20101013 / $I:(DE-82)080011_20140620$},
      pnm          = {899 - ohne Topic (POF4-899)},
      pid          = {G:(DE-HGF)POF4-899},
      typ          = {PUB:(DE-HGF)16},
      UT           = {WOS:000480295100006},
      doi          = {10.1016/j.matpr.2019.05.285},
      url          = {https://juser.fz-juelich.de/record/901964},
}