000908632 1001_ $$0P:(DE-HGF)0$$aF, Kullmann$$b0$$eCorresponding author
000908632 1112_ $$a15th European SOFC and SOE Forum$$cLucerne$$d2022-07-05 - 2022-07-08$$gEFCF2022$$wSwitzerland
000908632 245__ $$aSulfur poisoning of Ni/CGO fuel electrodes at low operating temperature
000908632 260__ $$c2022
000908632 3367_ $$033$$2EndNote$$aConference Paper
000908632 3367_ $$2BibTeX$$aINPROCEEDINGS
000908632 3367_ $$2DRIVER$$aconferenceObject
000908632 3367_ $$2ORCID$$aCONFERENCE_POSTER
000908632 3367_ $$2DataCite$$aOutput Types/Conference Poster
000908632 3367_ $$0PUB:(DE-HGF)24$$2PUB:(DE-HGF)$$aPoster$$bposter$$mposter$$s1661146634_5165$$xAfter Call
000908632 536__ $$0G:(DE-HGF)POF4-1231$$a1231 - Electrochemistry for Hydrogen (POF4-123)$$cPOF4-123$$fPOF IV$$x0
000908632 536__ $$0G:(DE-Juel1)SOFC-20140602$$aSOFC - Solid Oxide Fuel Cell (SOFC-20140602)$$cSOFC-20140602$$fSOFC$$x1
000908632 7001_ $$0P:(DE-Juel1)189092$$aJuckel, Martin$$b1
000908632 7001_ $$0P:(DE-HGF)0$$aWeber, A.$$b2
000908632 909CO $$ooai:juser.fz-juelich.de:908632$$pVDB
000908632 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)189092$$aForschungszentrum Jülich$$b1$$kFZJ
000908632 9131_ $$0G:(DE-HGF)POF4-123$$1G:(DE-HGF)POF4-120$$2G:(DE-HGF)POF4-100$$3G:(DE-HGF)POF4$$4G:(DE-HGF)POF$$9G:(DE-HGF)POF4-1231$$aDE-HGF$$bForschungsbereich Energie$$lMaterialien und Technologien für die Energiewende (MTET)$$vChemische Energieträger$$x0
000908632 9141_ $$y2022
000908632 920__ $$lyes
000908632 9201_ $$0I:(DE-Juel1)IEK-1-20101013$$kIEK-1$$lWerkstoffsynthese und Herstellungsverfahren$$x0
000908632 980__ $$aposter
000908632 980__ $$aVDB
000908632 980__ $$aI:(DE-Juel1)IEK-1-20101013
000908632 980__ $$aUNRESTRICTED
000908632 981__ $$aI:(DE-Juel1)IMD-2-20101013