001     1034990
005     20250610131445.0
024 7 _ |a 10.1002/aenm.202404569
|2 doi
024 7 _ |a 1614-6832
|2 ISSN
024 7 _ |a 1614-6840
|2 ISSN
024 7 _ |a 10.34734/FZJ-2025-00096
|2 datacite_doi
024 7 _ |a WOS:001385287700001
|2 WOS
037 _ _ |a FZJ-2025-00096
082 _ _ |a 050
100 1 _ |a Wang, Jian-Fen
|0 P:(DE-Juel1)199048
|b 0
|u fzj
245 _ _ |a Molecular Insights into the Interfacial Phenomena at the Li Metal | Polymer Solid‐State Electrolyte in Anode‐Free Configuration During Li Plating‐Stripping via Advanced Operando ATR‐FTIR Spectroscopy
260 _ _ |a Weinheim
|c 2025
|b Wiley-VCH
336 7 _ |a article
|2 DRIVER
336 7 _ |a Output Types/Journal article
|2 DataCite
336 7 _ |a Journal Article
|b journal
|m journal
|0 PUB:(DE-HGF)16
|s 1749210128_30448
|2 PUB:(DE-HGF)
336 7 _ |a ARTICLE
|2 BibTeX
336 7 _ |a JOURNAL_ARTICLE
|2 ORCID
336 7 _ |a Journal Article
|0 0
|2 EndNote
500 _ _ |a German Federal Ministry for Education and Research within the project “EFoBatt” (grant number 13XP5129)
520 _ _ |a Solid-state batteries are regarded as safe and high-energy-density candidates for next-generation energy storage. However, gaining a mechanistic understanding of the interfacial phenomena under real electrochemically working conditions remains a major challenge for cells containing solid-state electrolytes. This work presents an in-house built attenuated total reflection fourier-transform infrared (ATR-FTIR) spectroscopy cell equipped with an internal temperature-control unit. This cell is used for operando characterization of interfacial processes between plated Li and polymer during Li plating/stripping. As a proof of concept, a polymer electrolyte (cr-PEO10LiTFSI) containing poly(ethylene oxide), Li bis-(trifluoromethanesulfonyl)imide and crosslink-initiator benzophenone (BP) is introduced on a copper mesh as current collector at 60 °C. The developed ATR-FTIR spectroscopy setup provides detailed insights into the electrolyte degradation and reveals the crystallinity transformation of PEO at the interface during plating. Moreover, for the first time, the degradation of BP is observed. This compound, often overlooked in electrolyte systems due to its low concentration, is found to play a significant role in the interfacial electrochemistry process. Overall, this study provides a comprehensive overview of the characterization on the PEO electrolyte-lithium metal interface and introduces a novel perspective on the reaction of BP as a crosslinking initiator in the solid-state batteries.
536 _ _ |a 1221 - Fundamentals and Materials (POF4-122)
|0 G:(DE-HGF)POF4-1221
|c POF4-122
|f POF IV
|x 0
588 _ _ |a Dataset connected to DataCite
700 1 _ |a Weiling, Matthias
|0 P:(DE-Juel1)190810
|b 1
700 1 _ |a Pfeiffer, Felix
|0 P:(DE-Juel1)188450
|b 2
700 1 _ |a Liu, Kun-Ling
|0 P:(DE-Juel1)178047
|b 3
700 1 _ |a Baghernejad, Masoud
|0 0000-0002-2754-6623
|b 4
|e Corresponding author
773 _ _ |a 10.1002/aenm.202404569
|g p. 2404569
|0 PERI:(DE-600)2594556-7
|n 8
|p 2404569
|t Advanced energy materials
|v 15
|y 2025
|x 1614-6832
856 4 _ |u https://juser.fz-juelich.de/record/1034990/files/Advanced%20Energy%20Materials%20-%202025%20-%20Wang%20-%20Molecular%20Insights%20into%20the%20Interfacial%20Phenomena%20at%20the%20Li%20Metal%20Polymer.pdf
|y OpenAccess
909 C O |o oai:juser.fz-juelich.de:1034990
|p openaire
|p open_access
|p OpenAPC_DEAL
|p driver
|p VDB
|p openCost
|p dnbdelivery
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 0
|6 P:(DE-Juel1)199048
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 1
|6 P:(DE-Juel1)190810
910 1 _ |a Forschungszentrum Jülich
|0 I:(DE-588b)5008462-8
|k FZJ
|b 2
|6 P:(DE-Juel1)188450
913 1 _ |a DE-HGF
|b Forschungsbereich Energie
|l Materialien und Technologien für die Energiewende (MTET)
|1 G:(DE-HGF)POF4-120
|0 G:(DE-HGF)POF4-122
|3 G:(DE-HGF)POF4
|2 G:(DE-HGF)POF4-100
|4 G:(DE-HGF)POF
|v Elektrochemische Energiespeicherung
|9 G:(DE-HGF)POF4-1221
|x 0
914 1 _ |y 2025
915 p c |a APC keys set
|0 PC:(DE-HGF)0000
|2 APC
915 p c |a DEAL: Wiley 2019
|0 PC:(DE-HGF)0120
|2 APC
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0150
|2 StatID
|b Web of Science Core Collection
|d 2023-10-26
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0160
|2 StatID
|b Essential Science Indicators
|d 2023-10-26
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)1160
|2 StatID
|b Current Contents - Engineering, Computing and Technology
|d 2023-10-26
915 _ _ |a Creative Commons Attribution CC BY 4.0
|0 LIC:(DE-HGF)CCBY4
|2 HGFVOC
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0600
|2 StatID
|b Ebsco Academic Search
|d 2023-10-26
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)1150
|2 StatID
|b Current Contents - Physical, Chemical and Earth Sciences
|d 2023-10-26
915 _ _ |a DEAL Wiley
|0 StatID:(DE-HGF)3001
|2 StatID
|d 2023-10-26
|w ger
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0200
|2 StatID
|b SCOPUS
|d 2023-10-26
915 _ _ |a WoS
|0 StatID:(DE-HGF)0113
|2 StatID
|b Science Citation Index Expanded
|d 2023-10-26
915 _ _ |a OpenAccess
|0 StatID:(DE-HGF)0510
|2 StatID
915 _ _ |a Peer Review
|0 StatID:(DE-HGF)0030
|2 StatID
|b ASC
|d 2023-10-26
915 _ _ |a JCR
|0 StatID:(DE-HGF)0100
|2 StatID
|b ADV ENERGY MATER : 2022
|d 2023-10-26
915 _ _ |a IF >= 25
|0 StatID:(DE-HGF)9925
|2 StatID
|b ADV ENERGY MATER : 2022
|d 2023-10-26
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0300
|2 StatID
|b Medline
|d 2023-10-26
915 _ _ |a DBCoverage
|0 StatID:(DE-HGF)0199
|2 StatID
|b Clarivate Analytics Master Journal List
|d 2023-10-26
920 1 _ |0 I:(DE-Juel1)IMD-4-20141217
|k IMD-4
|l Helmholtz-Institut Münster Ionenleiter für Energiespeicher
|x 0
980 _ _ |a journal
980 _ _ |a VDB
980 _ _ |a UNRESTRICTED
980 _ _ |a I:(DE-Juel1)IMD-4-20141217
980 _ _ |a APC
980 1 _ |a APC
980 1 _ |a FullTexts


LibraryCollectionCLSMajorCLSMinorLanguageAuthor
Marc 21