000838473 1001_ $$0P:(DE-HGF)0$$aFriesen, Alex$$b0
000838473 245__ $$aInfluence of temperature on the aging behavior of 18650-type lithium ion cells: A comprehensive approach combining electrochemical characterization and post-mortem analysis
000838473 260__ $$aNew York, NY [u.a.]$$bElsevier$$c2017
000838473 3367_ $$2DRIVER$$aarticle
000838473 3367_ $$2DataCite$$aOutput Types/Journal article
000838473 3367_ $$0PUB:(DE-HGF)16$$2PUB:(DE-HGF)$$aJournal Article$$bjournal$$mjournal$$s1508390805_24788
000838473 3367_ $$2BibTeX$$aARTICLE
000838473 3367_ $$2ORCID$$aJOURNAL_ARTICLE
000838473 3367_ $$00$$2EndNote$$aJournal Article
000838473 520__ $$aThe understanding of the aging behavior of lithium ion batteries in automotive and energy storage applications is essential for the acceptance of the technology. Therefore, aging experiments were conducted on commercial 18650-type state-of-the-art cells to determine the influence of the temperature during electrochemical cycling on the aging behavior of the different cell components. The cells, based on Li(Ni0.5Co0.2Mn0.3)O2 (NCM532)/graphite, were aged at 20 °C and 45 °C to different states of health. The electrochemical performance of the investigated cells shows remarkable differences depending on the cycling temperature. At contrast to the expected behavior, the cells cycled at 45 °C show a better electrochemical performance over lifetime than the cells cycled at 20 °C. Comprehensive post-mortem analyses revealed the main aging mechanisms, showing a complex interaction between electrodes and electrolyte. The main aging mechanisms of the cells cycled at 45 °C differ strongly at contrast to cells cycled at 20 °C. A strong correlation between the formed SEI, the electrolyte composition and the electrochemical performance over lifetime was observed.
000838473 536__ $$0G:(DE-HGF)POF3-131$$a131 - Electrochemical Storage (POF3-131)$$cPOF3-131$$fPOF III$$x0
000838473 588__ $$aDataset connected to CrossRef
000838473 7001_ $$0P:(DE-HGF)0$$aMönnighoff, Xaver$$b1
000838473 7001_ $$0P:(DE-HGF)0$$aBörner, Markus$$b2
000838473 7001_ $$0P:(DE-HGF)0$$aHaetge, Jan$$b3
000838473 7001_ $$00000-0002-3743-8837$$aSchappacher, Falko M.$$b4$$eCorresponding author
000838473 7001_ $$0P:(DE-Juel1)166130$$aWinter, Martin$$b5$$eCorresponding author$$ufzj
000838473 773__ $$0PERI:(DE-600)1491915-1$$a10.1016/j.jpowsour.2016.12.040$$gVol. 342, p. 88 - 97$$p88 - 97$$tJournal of power sources$$v342$$x0378-7753$$y2017
000838473 8564_ $$uhttps://juser.fz-juelich.de/record/838473/files/1-s2.0-S0378775316317360-main.pdf$$yRestricted
000838473 8564_ $$uhttps://juser.fz-juelich.de/record/838473/files/1-s2.0-S0378775316317360-main.gif?subformat=icon$$xicon$$yRestricted
000838473 8564_ $$uhttps://juser.fz-juelich.de/record/838473/files/1-s2.0-S0378775316317360-main.jpg?subformat=icon-1440$$xicon-1440$$yRestricted
000838473 8564_ $$uhttps://juser.fz-juelich.de/record/838473/files/1-s2.0-S0378775316317360-main.jpg?subformat=icon-180$$xicon-180$$yRestricted
000838473 8564_ $$uhttps://juser.fz-juelich.de/record/838473/files/1-s2.0-S0378775316317360-main.jpg?subformat=icon-640$$xicon-640$$yRestricted
000838473 8564_ $$uhttps://juser.fz-juelich.de/record/838473/files/1-s2.0-S0378775316317360-main.pdf?subformat=pdfa$$xpdfa$$yRestricted
000838473 909CO $$ooai:juser.fz-juelich.de:838473$$pVDB
000838473 9101_ $$0I:(DE-588b)5008462-8$$6P:(DE-Juel1)166130$$aForschungszentrum Jülich$$b5$$kFZJ
000838473 9131_ $$0G:(DE-HGF)POF3-131$$1G:(DE-HGF)POF3-130$$2G:(DE-HGF)POF3-100$$3G:(DE-HGF)POF3$$4G:(DE-HGF)POF$$aDE-HGF$$bEnergie$$lSpeicher und vernetzte Infrastrukturen$$vElectrochemical Storage$$x0
000838473 9141_ $$y2017
000838473 915__ $$0StatID:(DE-HGF)0100$$2StatID$$aJCR$$bJ POWER SOURCES : 2015
000838473 915__ $$0StatID:(DE-HGF)0200$$2StatID$$aDBCoverage$$bSCOPUS
000838473 915__ $$0StatID:(DE-HGF)0300$$2StatID$$aDBCoverage$$bMedline
000838473 915__ $$0StatID:(DE-HGF)0310$$2StatID$$aDBCoverage$$bNCBI Molecular Biology Database
000838473 915__ $$0StatID:(DE-HGF)0600$$2StatID$$aDBCoverage$$bEbsco Academic Search
000838473 915__ $$0StatID:(DE-HGF)0030$$2StatID$$aPeer Review$$bASC
000838473 915__ $$0StatID:(DE-HGF)0199$$2StatID$$aDBCoverage$$bThomson Reuters Master Journal List
000838473 915__ $$0StatID:(DE-HGF)0110$$2StatID$$aWoS$$bScience Citation Index
000838473 915__ $$0StatID:(DE-HGF)0150$$2StatID$$aDBCoverage$$bWeb of Science Core Collection
000838473 915__ $$0StatID:(DE-HGF)0111$$2StatID$$aWoS$$bScience Citation Index Expanded
000838473 915__ $$0StatID:(DE-HGF)1150$$2StatID$$aDBCoverage$$bCurrent Contents - Physical, Chemical and Earth Sciences
000838473 915__ $$0StatID:(DE-HGF)1160$$2StatID$$aDBCoverage$$bCurrent Contents - Engineering, Computing and Technology
000838473 915__ $$0StatID:(DE-HGF)9905$$2StatID$$aIF >= 5$$bJ POWER SOURCES : 2015
000838473 9201_ $$0I:(DE-Juel1)IEK-12-20141217$$kIEK-12$$lHelmholtz-Institut Münster Ionenleiter für Energiespeicher$$x0
000838473 980__ $$ajournal
000838473 980__ $$aVDB
000838473 980__ $$aI:(DE-Juel1)IEK-12-20141217
000838473 980__ $$aUNRESTRICTED
000838473 981__ $$aI:(DE-Juel1)IMD-4-20141217