Hauptseite > Publikationsdatenbank > Reduction of silicon dioxide interfacial layer to 4.6 A EOT by Al remote scavenging in high K/metal gate stacks on Si |
Journal Article | FZJ-2013-02206 |
; ; ; ; ; ; ; ; ; ; ; ;
2013
Elsevier
[S.l.] @
This record in other databases:
Please use a persistent id in citations: doi:10.1016/j.mee.2013.03.066
Abstract: The continued device scaling demands the reduction of the equivalent oxide thickness (EOT) below 1 nm. For HfO2-based gate stacks, the interfacial SiO2 limits the EOT scaling. A low EOT can only be achieved if the interfacial layer (IL) is reduced to its physical limit of ∼4 Å. Such thin EOT are achievable if redox reactions within the gate stack are employed in order to reduce SiO2. This study reports on the use of an Al layer in combination with a TiN metal electrode to reduce the IL and achieve lowest EOT values. The lowest EOT achieved was 4.6 Å. However, the scavenging process was found to strongly depend on the thermal budget after Al deposition. The presented process adapts a standard metal-inserted poly-Si flow (MIPS) prior to Al deposition, but may also be an option to control IL regrowth.
![]() |
The record appears in these collections: |