Abstract: A set of dedicated marker samples consisting of fine-grain graphite as substrate, an interlayer of 0.2–0.4 μm molybdenum (Mo) employed as marker, and a 5–10 μm thick carbon (C) marker layer on top were installed in Wendelstein 7-X (W7-X) to investigate locally the C erosion and deposition. In this study, a set of five individual marker tiles, installed in a vertical divertor element of the test divertor unit in half-module 50, and exposed to about 40 min of plasma predominant in the standard magnetic divertor configuration in the first year of divertor operation in W7-X (OP1.2A), were retrieved from the vessel for post-mortem analysis. Picosecond laser induced breakdown spectroscopy (ps-LIBS) was applied on these marker tiles in order to determine the local erosion/deposition pattern caused by plasma impact. The general erosion/deposition pattern on the vertical target element was studied with the aid of depth-profiling by Mo line emission due to ps-LIBS with the number of applied laser pulses (355 nm, 2.3 J cm−2, 35 ps) at one probing location. Several potential asymmetry factors which avoid a perfect layer-by-layer ablation process in the laser ablations are proposed and discussed when a rough layered structure sample with a rough surface is analysed by the ps-LIBS technique. Thereby, a simulation model was developed to correct the measurement error of the ps-LIBS method caused by the non-perfect rectangle profile of the applied laser beam. The depth resolution of the applied ps-LIBS system was determined by quantification of the laser ablation rates of the different layers and the C substrate which were measured utilising profilometry and cross comparison with the thicknesses of the C and Mo marker layers determined by a combined focused ion beam and scanning electron microscopy technique. For the first time, the erosion/deposition pattern on the vertical target was mapped and quantified by ps-LIBS technique. A relatively wide net erosion zone with a poloidal extend of about 200 mm was identified which can be correlated to the main particle interaction zone at the magnetic strike-line of the dominantly applied standard magnetic divertor configuration. At the position of peak erosion, not only 7.6 × 1019 C atoms/cm2 but also 2 × 1018 Mo atoms/cm2 which results can be extrapolated to total 15 × 1019 C atoms/cm2, were eroded due to plasma fuel particle (H, He) and impurity (O, C) ion impact.

Classification:

Contributing Institute(s):
  1. Plasmaphysik (IEK-4)
Research Program(s):
  1. 134 - Plasma-Wand-Wechselwirkung (POF4-134) (POF4-134)

Appears in the scientific report 2021
Database coverage:
Embargoed OpenAccess ; Clarivate Analytics Master Journal List ; Current Contents - Physical, Chemical and Earth Sciences ; Ebsco Academic Search ; Essential Science Indicators ; IF < 5 ; JCR ; National-Konsortium ; NationallizenzNationallizenz ; SCOPUS ; Science Citation Index Expanded ; Web of Science Core Collection
Click to display QR Code for this record

The record appears in these collections:
Document types > Articles > Journal Article
Institute Collections > IFN > IFN-1
Workflow collections > Public records
IEK > IEK-4
Publications database
Open Access

 Record created 2021-03-24, last modified 2024-07-11


Published on 2020-12-08. Available in OpenAccess from 2021-12-08.:
Download fulltext PDF
(additional files)
External link:
Download fulltextFulltext by OpenAccess repository
Rate this document:

Rate this document:
1
2
3
 
(Not yet reviewed)